LOCTITE EA 9895

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9895

Main features

  • One-Piece Peel-Ply Removal
  • Bond-Ready Surface Without Sanding
  • 177 deg C Prepreg Co-Cure

Product Description

LOCTITE EA 9895 WPP AERO is a one-part polyester wet peel ply film for preparing composite bond surfaces during co-cure. The off-white film has a nominal areal weight of 161 g/m^2, 48% resin content and a polyester peel-ply carrier. After cure and removal, it leaves a clean surface ready for the next bonding step without sanding or solvent wiping. The fabric strips in one piece, supporting efficient processing on large composite parts. The film cures for 90 to 120 minutes at 177 deg C and is compatible with composite prepreg resin systems.

Key features

  • One-piece peel removal: The cured fabric strips in one piece to reduce removal time.
  • Bond-ready surface: Removal leaves a clean surface ready for the next bonding step without sanding or solvent wiping.
  • Prepreg co-cure processing: The film cures at 177 deg C and is compatible with composite prepreg resin systems.

Applications

Applications include composite bond-surface preparation and wet peel-ply processing with compatible composite prepreg resin systems.

Technical Specifications

General Properties
Color
The color
Neutral-off white
Other Properties
Storage Temperature
-18° °C

Additional Information

Technical properties

As-supplied properties

Product details for the one-part wet peel ply film.

Property Value Unit Method / condition
Product formOne-part filmWet peel ply
Areal weight161g/m^20.033 lb/sf
Support carrierPolyester peel plyAs supplied
Roll dimensionsNominal 1 m x 50.9 m3 ft x 167 linear ft
Resin content48%Nominal
Storage temperature-18 or belowdeg CCold storage
Open assembly timeAt least 14daysAt 25 deg C
Open assembly timeAt least 7daysAt 32 deg C
Technical properties

Final-state properties

Characteristics after cure and peel-ply removal.

Property Value Unit Method / condition
Removal behaviorStrips in one pieceAfter cure
Bond-surface conditionClean and ready for bondingAfter fabric removal
Residual polyester fibersMinimalAfter removal
Additional surface preparationNot requiredNo sanding or solvent wiping

Leading Brands Trust in Our Products and Services