LOCTITE EA 9891RP

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9891RP

Main features

  • Visual Color-Change Mix Verification
  • Room-Temperature Abradable Seal Repair
  • Abrasion-Resistant Paste Restoration

Product Description

LOCTITE EA 9891RP AERO is a two-component, room-temperature-curing epoxy repair paste for restoring LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials. The abrasion-resistant paste is applied to localized worn or damaged areas, and a color-change mixing indicator confirms uniform blending of Parts A and B. The paste supports controlled placement on abradable surfaces, while room-temperature cure limits the need for elevated-temperature processing. Its application scope is the 9890 abradable-seal repair system and related paste repairs.

Key features

  • Visual mix confirmation: A color-change indicator helps confirm uniform blending of the two components.
  • Room-temperature repair cure: The epoxy paste cures at room temperature for localized repair processing.
  • Abrasion-resistant restoration: The repair paste restores LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials.

Applications

Applications include repair of LOCTITE EF 9890 AERO and SynSpand 9890 abradable seal materials.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (A / B)
Density (g)
0.7 / 0.5 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100: 40
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
20 minutes minutes