Loctite EA 9837.1 030OST AERO

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9837.1 030OST AERO

Main features

  • Long-Open-Time Composite Surfacing
  • Fast 121/177 deg C Cure
  • High-Adhesion Composite Surface Film

Product Description

LOCTITE EA 9837.1 AERO is an epoxy-based composite surfacing film designed for aerospace composite structures and honeycomb-stiffened composite parts. Available in 0.030 psf (150 g/m²) and 0.035 psf (170 g/m²) formats, it is engineered to improve surface quality while minimizing core crush and porosity during composite fabrication. The film is co-curable with composite prepregs and supports cure schedules at either 250°F (121°C) or 350°F (177°C). Its paintable surface, resistance to microcracking, and compatibility with lightning strike screens and foils make it suitable for aerospace composite components requiring enhanced surface finish and paint adhesion.

Key features

  • Composite Surfacing Film: Improves the surface quality of honeycomb-stiffened composite parts while minimizing porosity and core crush.
  • Co-Curable Epoxy System: Compatible with composite prepregs and can be cured at either 250°F (121°C) or 350°F (177°C).
  • Paintable Surface Quality: Provides a high-quality paintable surface with greater than 95% primer adhesion in cross-hatch paint adhesion testing.

Applications / Suitable for

  • Honeycomb-stiffened composite structures
  • Aerospace composite parts requiring improved surface finish
  • Composite components requiring paint-ready surfaces
  • Co-cure processing with aerospace prepregs
  • Applications utilizing lightning strike screens and foils

Technical Specifications

General Properties
Color
The color
Opaque Gray

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for LOCTITE EA 9837.1 AERO composite surfacing film.

Property Value Unit Method / condition
Color Opaque Gray - Visual examination
Available Weight 150 or 170 g/m² Nominal film weight
Gel Time 20 - 35 minutes At 250°F (121°C)
Gel Time 0.5 - 2 minutes At 350°F (177°C)
Volatiles 1.5 % Maximum typical value
Open Assembly Time At least 21 days 77°F (25°C)
Shelf Life 12 months Stored at 0°F (-18°C) or below
Technical properties

After-processing / final-state properties

Representative cured-system and performance data.

Property Value Unit Method / condition
Primer Adhesion >95 % Initial, no exposure, cross-hatch paint adhesion
Primer Adhesion >95 % After 7 days deionized water exposure at 25°C
Cure Schedule 2 hours 250°F (121°C) cure, 45 psi pressure
Alternative Cure Schedule 1.5 hours 350°F (177°C) cure, 45 psi pressure