LOCTITE EA 9825

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9825

Main features

  • Low-Density, One-Component Epoxy Syntactic
  • Up to 350 deg F Service
  • Honeycomb Composite Potting

Product Description

LOCTITE® EA 9825 AERO is a low-density, one-component epoxy syntactic for honeycomb composite parts requiring high compressive strength at temperatures up to 350°F (177°C). The paste material is suitable for localized filling and reinforcement applications where weight and cured compression performance are important. It supports cure schedules at either 250°F (121°C) or 350°F (177°C), allowing integration with different heated aerospace composite processes. Documented uses include fastener or attachment potting and reinforcement of panel edges.

Key features

  • Low-density epoxy syntactic: The cured material has a typical density of 0.72 g/cc.
  • High compressive strength: Supports reinforced honeycomb composite structures and localized potting applications.
  • Dual cure schedules: May be cured at 250°F (121°C) or 350°F (177°C) using the documented thermal profiles.

Applications / Suitable for

  • Honeycomb composite parts
  • Fastener or attachment potting
  • Panel-edge reinforcement

Technical Specifications

General Properties
Color
The color
Amber
Density
Volumetric mass per unit
720 kg/m3
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical handling and storage properties for the one-component epoxy syntactic.

Property Value Unit Method / condition
Color Amber — As supplied
Extrusion rate 1,000 g/min At 77°F (25°C), following the documented conditioning procedure
Work life after thaw 8 hours At 77°F (25°C)
Shelf life 12 months Stored at 10°F (-12°C) or below

After-processing / final-state properties

Typical cured density and compressive properties. Compression values depend on cure schedule, specimen geometry, and test temperature.

Property Value Unit Method / condition
Cured density 0.72 g/cc Typical cured value
Compressive strength, 2% offset 10.7 / 73.8 ksi / MPa ASTM D695; cured at 250°F (121°C); tested at 77°F (25°C); Test 1 specimen
Ultimate compressive strength 13.3 / 91.7 ksi / MPa ASTM D695; cured at 250°F (121°C); tested at 77°F (25°C); Test 1 specimen
Ultimate compressive strength 8.6 / 59.3 ksi / MPa ASTM D695; cured at 350°F (177°C); tested at 300°F (149°C); Test 1 specimen
Ultimate compressive strength 7.2 / 49.7 ksi / MPa ASTM D695; cured at 350°F (177°C); tested at 350°F (177°C); Test 2 specimen