LOCTITE EA 9807

Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm

LOCTITE EA 9807

Main features

  • Pourable Intermediate-Density Epoxy Syntactic
  • Room-Temperature or Heat Cure
  • 121 deg C Service Temperature

Product Description

LOCTITE® EA 9807 AERO is a two-part, intermediate-density structural epoxy syntactic potting compound for potting and edge-filling honeycomb assembly parts and repair areas. The purple mixed material has a pourable consistency and a 90-minute pot life for a 100 g mass at 25°C. It cures at room temperature or may be heat cured after a minimum 60-minute ambient gel period. The formulation combines flame-retardant characteristics, controlled exotherm and cured mechanical performance for aerospace honeycomb assembly applications. Its defined service temperature is 121°C (250°F), based on retaining 6.9 MPa (1,000 psi) lap shear strength under ASTM D1002.

Key features

  • Pourable syntactic epoxy: Supports controlled placement in potting and edge-fill areas.
  • Flexible cure options: Cures in 5 to 7 days at 25°C or may be heat cured after a minimum 60-minute ambient gel period.
  • High-temperature capability: Has a defined service temperature of 121°C (250°F) based on ASTM D1002 lap shear performance.

Applications / Suitable for

  • Potting honeycomb assembly parts
  • Honeycomb edge filling
  • Honeycomb assembly repair applications
Product Family

LOCTITE EA 9807

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Purple (Resin) / Amber (Epoxy) / Purple (Mixed)
Density
Volumetric mass per unit
960 kg/m3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:29.6 (by weight)
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
ASTM D7028 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed material before cure.

Property Value Method / condition
Components Two components Requires mixing
Appearance Resin: purple
Hardener: amber
Mixed: purple
As supplied and mixed
Mix ratio 100:29.6 Resin:hardener by weight
Resin density 0.82 g/cm³ Part A
Hardener density 0.96 g/cm³ Part B
Mixed density 0.85 g/mL Mixed material
Mixed viscosity 14,194 mPa·s (cP) Brookfield-RVT at 25°C; spindle 6, 20 rpm
Pot life 90 minutes 100 g mass at 25°C (77°F), in water bath; ASTM D2471
Recommended cure 5 days at 25°C (77°F)
90 minutes at 127°C (260°F)
60 minutes at 177°C (350°F)
Elevated-temperature cures require a minimum 60-minute ambient gel period before heat exposure

After-processing / final-state properties

Typical cured-material properties. Results depend on the stated cure schedule, specimen and test conditions.

Property Value Method / condition
Shore hardness 70 Shore D Cured 5 days at 25°C (77°F); approximately 6.35 mm (0.25 in) thick
Glass-transition temperature, Tg 67°C (153°F)
112°C (233°F)
107°C (225°F)
116°C (241°F)
ASTM D7028, dry E′; respectively cured 7 days at 25°C, 90 minutes at 127°C, 60 minutes at 177°C, and 14 days at 177°C
Coefficient of thermal expansion CTE 1: 52.9 µm/m·°C
CTE 2: 101.7 µm/m·°C
ASTM E831-05; cured 7 days at 25°C; CTE 1 before Tg and CTE 2 after Tg
Tensile lap shear strength 28.8 N/mm² (4,175 psi)
27.8 N/mm² (4,025 psi)
27.5 N/mm² (3,990 psi)
ASTM D1002 / EN 2243-1 at 25°C; 2024-T3 clad aluminum, phosphoric-acid anodized, 10 mil bondline; respectively cured 7 days at 25°C, 60 minutes at 177°C and 14 days at 177°C
Compression ultimate strength at 25°C 73.5 MPa (10.7 ksi)
86.2 MPa (12.5 ksi)
98.9 MPa (14.3 ksi)
ASTM D695 / ISO 604; respectively cured 7 days at 25°C, 60 minutes at 177°C and 14 days at 177°C
Service temperature 121°C (250°F) Defined as the temperature at which the adhesive retains 6.9 MPa (1,000 psi) under ASTM D1002