LOCTITE EA 9658.060UNS

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9658.060UNS

Main features

  • Unsupported 0.060 lb/sf Film
  • 177 deg C Cure Capability
  • Extended 15-Day Assembly Window

Product Description

LOCTITE EA 9658.060 PSF UNS AERO is the 0.060 lb/sf unsupported configuration of the high-temperature EA 9658 epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The UNS construction contains no fabric carrier and cures for 1 hour at 177 deg C under maintained pressure. Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C, while refrigerated storage at -18 deg C or below provides a 9-month warranty life. Applications include high-temperature aerospace structures requiring the specified unsupported film configuration.

Key features

  • Unsupported film construction: The 0.060 lb/sf UNS configuration contains no fabric carrier.
  • High-temperature cure: The film cures for 1 hour at 177 deg C under maintained pressure.
  • Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.

Applications

Applications include nacelle metal, composite and honeycomb bonding where the 0.060 lb/sf unsupported construction is specified.

Product Family

LOCTITE EA 9658.060UNS

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
≤ -18 °C °C
General Properties
Density
Volumetric mass per unit
0.72 kg/m3

Additional Information

Technical properties

As-supplied properties

Configuration-specific and common family handling values.

Property Value Unit Method / condition
ConfigurationEA 9658 .060 PSF UNSSpecific product variant
ConstructionUnsupported adhesiveNo fabric carrier
Standard package36 in x 150 ft450 sf roll
Open assembly timeAt least 15daysAt 25 deg C
Open assembly timeAt least 10daysAt 32 deg C
Storage temperature-18 or belowdeg CSealed container
Warranty life9monthsAt -18 deg C or below, from shipment
Cure schedule1 hour at 177 deg CHeat-up rate 2.2 to 4 deg C/minute