LOCTITE EA 9658

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9658

Main features

  • 177 deg C Nacelle Bonding
  • Extended 15-Day Assembly Window
  • Controlled Flow and Flash

Product Description

LOCTITE EA 9658 AERO is a high-temperature epoxy film adhesive for nacelle metal, composite and honeycomb bonding. The family is offered in unsupported and nonwoven-glass-supported constructions, including 0.060, 0.065 and 0.100 lb/sf configurations. It cures for 1 hour at 177 deg C and is intended for continuous exposure up to 177 deg C, with thermal stability extending to 6,000 hours at that temperature. Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C. Applications include high-temperature nacelle and aerospace structural bonding.

Key features

  • High-temperature cure: The film cures for 1 hour at 177 deg C.
  • Extended assembly window: Open assembly time is at least 15 days at 25 deg C or 10 days at 32 deg C.
  • Controlled adhesive flow: The film is formulated for flow control that limits hole blockage and excess flash.

Applications

Applications include nacelle metal, composite and honeycomb bonding where continuous exposure up to 177 deg C is required.

Technical Specifications

Other Properties
Storage Temperature
≤18 °C

Additional Information

Technical properties

As-supplied properties

Family-level configuration and handling values.

Property Value Unit Method / condition
Construction optionsUnsupported or nonwoven-glass-supportedUNS or NWG configurations
Film configurations0.060, 0.065 or 0.100lb/sfConfiguration-dependent
Standard package36 in x 150 ft450 sf roll
Open assembly timeAt least 15daysAt 25 deg C
Open assembly timeAt least 10daysAt 32 deg C
Storage temperature-18 or belowdeg CSealed container
Warranty life9monthsAt -18 deg C or below, from shipment
Cure schedule1 hour at 177 deg CHeat-up rate 2.2 to 4 deg C/minute

Leading Brands Trust in Our Products and Services