LOCTITE EA 9394.3

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9394.3

Main features

  • 4,200 psi Aluminum Lap Shear
  • 90-Minute Working Window
  • Thixotropic Gap-Filling Control

Product Description

LOCTITE EA 9394.3 AERO is a two-part structural epoxy paste adhesive that cures at room temperature and is formulated for bonded assemblies requiring controlled bondline thickness and elevated-temperature performance. Its thixotropic, gap-filling consistency supports structural bonding, potting, filling and liquid-shim work, while 5 mil glass beads help control the bondline. The mixed adhesive has a typical 90-minute pot life at 25°C for a 450 g mass. Typical ASTM D1002 lap-shear testing on phosphoric-acid-anodized 2024-T3 aluminum shows 4,200 psi at 25°C and 1,200 psi at 177°C.

Key features

  • Elevated-temperature lap shear: Typical tensile lap shear is 1,200 psi (8.3 MPa) at 177°C under the stated aluminum test configuration.
  • Controlled bondline: The formulation contains 5 mil glass beads to help establish bondline thickness.
  • Extended pot life: Typical pot life is 90 minutes at 25°C for a 450 g mixed mass.
  • Room-temperature or accelerated cure: Cure for 3–5 days at 25°C, or use 1 hour at 66°C for complete cure; accelerated cure is limited to small masses.
  • Thixotropic gap filling: The paste consistency supports potting, filling and liquid-shim applications.

Applications / Suitable for

  • Structural bonding of properly prepared aluminum assemblies
  • Potting and cavity filling
  • Liquid shimming and controlled-gap bonding

Technical Specifications

General Properties
Color
The color
Gray (Part A) / Black (Part B) / Gray (Mixed)
Density (g)
1.50 (Part A) / 1.00 (Part B) g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:17
Physical Properties
Viscosity (Part A)
400,000 to 800,000 mPa.s
Viscosity (Part B)
20,000 to 70,000 mPa.s

Additional Information

Structural epoxy adhesive

LOCTITE EA 9394.3 AERO

LOCTITE EA 9394.3 AERO is a two-part, room-temperature-curing structural epoxy paste for assemblies that require controlled bondline thickness, gap filling and retained strength at elevated temperature. The thixotropic mixed adhesive contains 5 mil glass beads and provides a typical 90-minute pot life at 25°C for a 450 g mass.

Two-part epoxy paste Room-temperature cure Thixotropic gap filling 90-minute pot life at 25°C 5 mil bondline-control beads 177°C service temperature

 

As supplied

Uncured properties

Typical component and mixed-material values. Viscosity data are method- and temperature-specific and should not be compared without preserving the stated Brookfield conditions.

Property Value Unit Method / condition
Color Part A: gray; Part B: black; mixed: gray — As supplied and immediately after mixing
Viscosity at 25°C Part A: 400–800; Part B: 20–70; mixed: 160 Pa·s Brookfield HBT; Part A spindle 7, Part B spindle 4 and mixed spindle 5 at 2.09 rad/s
Density Part A: 1.50; Part B: 1.00; mixed: 1.36 g/mL Typical as-supplied values
Shelf life 1 year for Part A and Part B — Stored below 25°C
Bondline-control beads 5 mil Glass beads contained in the mixed adhesive
Physical form and rheology Thixotropic paste — Two-component structural epoxy adhesive
Processing

Mixing, application and cure

Process control is important for ratio accuracy, mixed-mass temperature, bondline formation and cure development. Keep working-time, handling-strength and full-cure stages distinct when planning assembly loads.

Mix ratio: Combine Part A and Part B at 100:17 by weight and mix thoroughly. Volume measurement is not recommended for structural applications unless the ratio is controlled by special precautions.
Batch size and pot life: Typical pot life is 90 minutes at 25°C for a 450 g mass. Do not mix more than 450 g because larger mixed masses can generate hazardous exotherm and toxic fumes.
Surface preparation and assembly: Use clean, dry and properly prepared bonding surfaces. Apply the mixed adhesive, assemble the parts and maintain contact or support until the adhesive has set.
Handling strength: Handling strength develops after 24 hours at 25°C. Support tooling or pressure may then be removed, but full bond strength has not yet developed and applied loads should remain small.
Cure: Cure for 3–5 days at 25°C for normal performance. For small masses, accelerated cure may be used up to 93°C; 1 hour at 66°C provides complete cure.
Storage and Handling

Store Part A and Part B below 25°C; the stated shelf life is 1 year for each component. Keep containers tightly closed in a cool, well-ventilated location away from incompatible materials. Components should be near 25°C before mixing. Use appropriate ventilation and protective equipment, and do not heat unmixed Part A above 80°C or Part B above 100°C.

After cure

Cured material properties

Typical bulk-resin properties. These values describe cured material specimens and should not be treated as guaranteed bonded-joint design allowables.

Property Value Unit Method / condition
Tensile strength 6,675 psi (46.04 MPa) Typical at 25°C; ASTM D638 using 3.18 mm castings
Tensile modulus 0.615 × 106 psi (4,242 MPa) Typical at 25°C; ASTM D638 using 3.18 mm castings
Shear modulus, dry 212,000 psi (1,462 MPa) Typical at 25°C
Shear modulus, wet 148,500 psi (1,204 MPa) Typical at 25°C
Elongation at break 1.66 % Typical at 25°C
Shore D hardness 88 — Typical at 25°C
Glass transition temperature, dry 78 °C Typical bulk-resin value
Glass transition temperature, wet 68 °C Typical bulk-resin value
Performance evidence

Typical lap shear strength by test temperature

ASTM D1002 results after a 5-day cure at 25°C on phosphoric-acid-anodized 2024-T3 bare aluminum. Values are typical laboratory results for the stated specimen configuration.

Property Value Unit Method / condition
Tensile lap shear at −55°C 3,300 psi (22.8 MPa) ASTM D1002; 2024-T3 bare aluminum, phosphoric-acid anodized per ASTM D3933; 5-day cure at 25°C
Tensile lap shear at 25°C 4,200 psi (29.0 MPa) Same specimen preparation and cure
Tensile lap shear at 82°C 3,000 psi (20.7 MPa) Same specimen preparation and cure
Tensile lap shear at 93°C 2,900 psi (20.0 MPa) Same specimen preparation and cure
Tensile lap shear at 121°C 2,300 psi (15.9 MPa) Same specimen preparation and cure
Tensile lap shear at 149°C 1,600 psi (11.0 MPa) Same specimen preparation and cure
Tensile lap shear at 177°C 1,200 psi (8.3 MPa) Same specimen preparation and cure
Tensile lap shear at 204°C 600 psi (4.1 MPa) Same specimen preparation and cure

Environmental exposure and peel performance

The following results provide additional context for tensile lap shear after liquid exposure and for bell peel on prepared aluminum. They apply only to the stated specimens, conditioning and test methods.

Lap shear after 7-day liquid exposure
Typical tensile lap shear at 25°C was 4,100 psi (28.3 MPa) after water exposure, 4,000 psi (27.6 MPa) after isopropyl alcohol, 4,100 psi (28.3 MPa) after hydraulic oil and 4,200 psi (29.0 MPa) after JP-4 fuel. The room-temperature control was 4,300 psi (29.7 MPa).
Each exposure was 7 days at 25°C; results were tested at 25°C.
Bell peel and defined service temperature
Typical bell peel strength is 20 pli at 25°C. The defined service temperature is 177°C, based on retention of 1,000 psi (6.9 MPa) tensile lap shear using ASTM D1002.
Bell peel: ASTM D3167 after 7 days at 25°C on phosphoric-acid-anodized 2024-T3 clad aluminum.
Use contexts

Applications

The product combines structural bonding performance, thixotropic gap filling and built-in bondline control for several prepared-assembly use contexts.

Prepared aluminum structural assembly configured for adhesive bonding
Prepared aluminum structural bonding
ASTM D1002 testing on phosphoric-acid-anodized 2024-T3 aluminum provides bonded-joint strength data from −55°C through 204°C. The room-temperature cure and controlled bondline are relevant where the tested metal preparation and joint configuration can be reproduced.
Assembly cavity prepared for epoxy potting or gap filling
Potting and cavity filling
The thixotropic paste and gap-filling capability support potting and filling where the uncured material must remain positioned before cure. Mixed quantity must remain within the 450 g limit to control exotherm.
Close-up of a liquid-shim bondline controlled by glass-bead spacers
Liquid shimming and gap compensation
The 5 mil glass beads help establish bondline thickness while the thixotropic paste fills localized gaps between properly prepared mating surfaces. Assembly support should remain in place through the handling-strength stage, and service loads should wait for full cure.
Next steps

Evaluate LOCTITE EA 9394.3 AERO for your assembly

Krayden can help review mix-ratio control, batch size, cure selection, bondline requirements and the relevance of the aluminum lap-shear data to your assembly. Contact our team to discuss product selection, samples, processing questions or a qualification plan for your specific substrates and operating conditions.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers