LOCTITE EA 9394

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9394 LOCTITE EA9394

Main features

  • Two-Part Aerospace Structural Epoxy Paste
  • 177 deg C Service Temperature
  • MMM-A-132 Qualified Epoxy

Product Description

LOCTITE® EA 9394 AERO is a two-part, thixotropic epoxy paste adhesive for structural bonding, repair, potting, filling, and liquid-shim applications in aerospace assemblies. It cures at room temperature, provides a 90-minute typical pot life for a 450 g mass at 25°C, and may also be heat cured for faster processing. The adhesive has a defined service temperature of 177 °C based on retention of at least 6.9 MPa tensile lap shear strength under ASTM D1002 testing. It is qualified to MMM-A-132 Rev B, Type I, Class 3, Form 3, Group 1, providing a documented military-specification basis for evaluating the material for applicable structural adhesive uses.

Key features

  • Two-part structural epoxy paste: Thixotropic mixed material supports controlled application, gap filling, potting, filling, and liquid-shim use.
  • Flexible cure options: Develops normal performance after 3–5 days at 25 °C or may be fully cured in 1 hour at 66 °C for suitable small-mass applications.
  • 90-minute typical pot life: Measured for a 450 g mixed mass at 25 °C using ASTM D2471.
  • MMM-A-132 qualification: Qualified to Rev B, Type I, Class 3, Form 3, Group 1 for the specification-defined adhesive category and requirements.

Applications / Suitable for

  • Aerospace structural bonding and repair involving prepared metal and honeycomb assemblies.
  • Potting and filling where a thixotropic structural epoxy paste is required.
  • Liquid-shim and gap-filling applications evaluated under the applicable design, process, and qualification requirements.

Technical Specifications

General Properties
Color
The color
Part A: Gray | Part B: Black
Density (g)
Mixed: 1.36 g/cm3
Physical Properties
Viscosity (Part A)
400000–800000 mPa.s
Viscosity (Part B)
20000–70000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the separate components and mixed adhesive before cure.

Property Value Unit Method / condition
Color Part A: Gray; Part B: Black; Mixed: Gray - Uncured components and mixed adhesive
Viscosity Part A: 400–800; Part B: 20–70; Mixed: 160 Pa·s 25°C; Brookfield HBT, component-specific spindle at 2.09 rad/sec
Density Part A: 1.50; Part B: 1.00; Mixed: 1.36 g/ml Uncured components and mixed adhesive
Mix ratio 100:17 Parts by weight Part A:Part B; volume measurement is not recommended for structural applications
Pot life 90 minutes 450 g mass at 75°F/25°C; ASTM D2471 in water bath
Shelf life 1 year Part A and Part B stored below 77°F/25°C
Technical properties

After-processing / final-state properties

Typical cured-material and bonded-joint properties under the stated specimen, cure and test conditions.

Property Value Unit Method / condition
Tensile lap shear strength 4,200 / 28.9 psi / MPa ASTM D1002 at 77°F/25°C; cured 5 days at 77°F/25°C; phosphoric-acid-anodized 2024-T3 bare aluminum
Tensile lap shear strength at 350°F/177°C 1,200 / 8.3 psi / MPa ASTM D1002; cured 5 days at 77°F/25°C; phosphoric-acid-anodized 2024-T3 bare aluminum
Tensile strength 6,675 / 46.0 psi / MPa ASTM D638; 0.125 in/3.18 mm casting at 77°F/25°C
Compressive strength 10,000 / 68.9 psi / MPa ASTM D695 at 77°F/25°C; rectangular cured specimens
Shore D hardness 88 Shore D Cured bulk resin at 77°F/25°C
Glass transition temperature Dry: 172 / 78; Wet: 154 / 68 °F / °C Cured bulk resin; dry and wet conditions reported separately
Thermal conductivity 0.331 W/(m·K) Cured bulk-resin property
Volume resistivity 4.05 × 1013 ohm-cm Cured bulk-resin electrical property

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers