LOCTITE EA 9340

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 9340

Main features

  • Visual 1:1 Mix Confirmation
  • Extended 90-Minute Pot Life
  • High-Temperature Shear Retention

Product Description

LOCTITE EA 9340 is a two-part, general-purpose epoxy paste adhesive for bonding wood, metals, ceramics and most plastics where heat and chemical exposure are important. Part A and Part B mix 1:1 by weight or volume to a uniform gray paste, with a 90-minute pot life for a 100 g mass at 25 deg C. Handling strength develops in 6 to 8 hours at room temperature, and full cure can be reached in 24 hours at 25 deg C or accelerated with heat. The cured adhesive can be sanded, drilled and painted for finish work.

Key features

  • Visual 1:1 mixing: Green Part A and gray Part B mix 1:1 to a uniform gray paste.
  • Extended pot life: The mixed adhesive has a 90-minute pot life for a 100 g mass at 25 deg C.
  • High-temperature shear retention: Typical shear strength is 1,850 psi at 82 deg C after the stated cure on etched aluminum.

Applications

Applications include bonding wood, metals, ceramics and most plastics for general-purpose assemblies requiring heat and chemical resistance.

Technical Specifications

General Properties
Color
The color
Green / Grey
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (A / B)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1

Additional Information

Technical properties

As-supplied properties

Typical component and mixed-system values at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
Part A colorGreenAs supplied
Part B colorGrayAs supplied
Mixed colorGrayAfter complete mixing
ViscosityPastePart A, Part B and mixed system
Mix ratio1:1By weight or by volume
Pot life90minutes100 g mass at 25 deg C
Recommended storage range8 to 21deg CUnopened container in a cool, dry location
Technical properties

Final-state properties

Typical values after 3 days at 25 deg C unless otherwise stated.

Property Value Unit Method / condition
Shore hardnessGreater than 80Durometer DCured material
Shear strength2,100psiASTM D 1002, etched aluminum, tested at -40 deg F
Shear strength2,300psiASTM D 1002, etched aluminum, tested at 77 deg F
Shear strength1,850psiASTM D 1002, etched aluminum, tested at 180 deg F