LOCTITE EA 9330

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9330

Main features

  • High Aluminum Peel and Lap-Shear Strength
  • 60-Minute Working Window
  • Multi-Fluid and Salt-Spray Resistance

Product Description

LOCTITE EA 9330 is a two-component epoxy paste adhesive for aerospace bonding applications. The cream-colored mixed adhesive cures at room temperature and combines high peel strength with environmental resistance. A 100:33 Part A-to-Part B mix ratio by weight provides a 60-minute pot life at 25°C for a 100 g mass. Handling strength develops in 24 hours at 25°C, while normal performance is reached after a 5- to 7-day room-temperature cure; a 1-hour cure at 82°C is available for small masses. Typical lap-shear testing on chromic-acid-etched 2024-T3 AlClad aluminum produced 34.5 to 43.4 MPa at 25°C, depending on cure schedule.

Key features

  • Mix ratio and pot life: 100:33 Part A to Part B by weight, with a typical 60-minute pot life at 25°C for a 100 g mass.
  • Cure options: 5 to 7 days at 25°C for normal performance or 1 hour at 82°C for complete cure of small masses.
  • Handling strength: Develops in 24 hours at 25°C while bonded parts are held in contact.
  • Bondline tolerance: Typical lap-shear strength ranges from 35.8 to 28.2 MPa across tested bondlines from 0.10 to 1.27 mm after a 7-day cure at 25°C.
  • Peel performance: Typical T-peel strength is 156 N/25 mm after a 7-day cure at 25°C on chromic-acid-etched 2024-T3 AlClad aluminum.
  • Defined service temperature: 82°C, based on retaining 6.9 MPa tensile lap-shear strength under ASTM D1002 testing.

Technical Specifications

General Properties
Color
The color
Cream (Part A) / Amber (Part B) / Cream (Mixed)
Density (g)
1.16 (Part A) / 1.03 (Part B) g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:33 by weight
Physical Properties
Viscosity (Part A)
74,000 mPa.s
Viscosity (Part B)
1,100 mPa.s

Additional Information

Aerospace epoxy adhesive

LOCTITE EA 9330

LOCTITE EA 9330 is a two-part epoxy paste adhesive developed for aerospace bonding. It provides a 60-minute pot life at 25°C, cures at room temperature, and develops high peel and lap-shear performance on prepared aluminum. Testing also shows performance after water, humidity, hydraulic-fluid, fuel, and salt-spray exposure under the stated conditions.

Two-component epoxy paste 100:33 mix ratio by weight 60-minute pot life at 25°C Room-temperature cure 24-hour handling strength 82°C defined service temperature
LOCTITE EA 9330 two-component epoxy paste adhesive packaging.

LOCTITE EA 9330 two-component epoxy paste adhesive.

Uncured adhesive

As-Supplied Properties

Typical values for the individual components and mixed adhesive. Viscosity values are measured at 25°C using a Brookfield HBT viscometer.

Property Value Unit Method / condition
Part A color Cream — As supplied
Part B color Amber — As supplied
Mixed color Cream — After complete mixing
Part A viscosity 74 Pa·s 25°C; Brookfield HBT, spindle 5 at 0.5 rad/s (5 rpm)
Part B viscosity 1.1 Pa·s 25°C; Brookfield HBT, spindle 1 at 2.09 rad/s (20 rpm)
Part A density 1.16 g/mL As supplied
Part B density 1.03 g/mL As supplied
Mixed density 1.14 g/mL After complete mixing
Processing

Mixing and Cure

Prepare clean, dry bonding surfaces, mix the two components completely, apply within the stated pot-life window, maintain contact during cure, and select the cure schedule appropriate to the assembly and mixed mass.

Mix ratio: Combine 100 parts Part A with 33 parts Part B by weight and mix completely. Volume measurement is not recommended for structural applications unless proper ratio control is assured.
Pot life: 60 minutes at 25°C for a 100 g mixed mass, measured by ASTM D2471 in a water bath.
Mixed quantity: Do not mix quantities greater than 450 g. Larger masses can produce dangerous heat buildup, uncontrolled decomposition, and toxic fumes.
Surface and assembly: Use clean, dry, properly prepared bonding surfaces. Hold the bonded parts in contact until the adhesive is set.
Handling strength: Develops in 24 hours at 25°C. Keep applied loads small until full bond strength is reached.
Cure: Allow 5 to 7 days at 25°C for normal performance. For small masses, accelerated cures up to 93°C may be used; 1 hour at 82°C provides complete cure.
Storage and Handling

Keep both components tightly closed in a cool, well-ventilated area. Store Part B between 0 and 25°C. Shelf life is 1 year below 25°C for each component, and the material should be placed into its intended storage conditions after receipt.

Cured Properties

Service temperature
82°C
Defined as the temperature at which the adhesive retains 6.9 MPa tensile lap-shear strength under ASTM D1002 testing.
Glass transition temperature
57°C
Typical bulk-resin value after a 7-day cure at 25°C.
Hardness
Shore D 80
Typical cured bulk-resin hardness after a 7-day cure at 25°C.
Property Value Unit Method / condition
Tensile strength 38.6 MPa ASTM D638; 3.18 mm castings; cured 7 days at 25°C; tested at 25°C
Tensile modulus 2,646 MPa ASTM D638; 3.18 mm castings; cured 7 days at 25°C; tested at 25°C
Elongation at break 2.4 % ASTM D638; 3.18 mm castings; cured 7 days at 25°C; tested at 25°C
Shear modulus 965 MPa Bulk resin; cured 7 days at 25°C
Poisson’s ratio 0.41 — Bulk resin; cured 7 days at 25°C
Compressive strength 53.1 MPa ASTM D695; 12.7 mm castings; tested at 25°C
Compressive modulus 1,743 MPa ASTM D695; 12.7 mm castings; tested at 25°C
Dielectric constant 4.50 / 4.38 / 4.23 / 3.96 — 100 Hz / 1 kHz / 10 kHz / 100 kHz; ASTM D150
Dissipation factor 0.025 / 0.020 / 0.032 / 0.056 — 100 Hz / 1 kHz / 10 kHz / 100 kHz; ASTM D150
Volume resistivity 1.59 × 1014 Ω·cm 25°C; 500 V; 1 minute electrification
Surface resistivity 1.59 × 1014 Ω 25°C; 500 V; 1 minute electrification

Bond Strength and Environmental Performance

The following values are typical laboratory results and are specific to the stated adherends, surface preparation, cure schedules, test temperatures, and exposure conditions. They are not guaranteed design allowables.

Tensile lap-shear strength across test temperatures
Test temperature 7 days at 25°C 2 hours at 82°C 1 hour at 121°C
−55°C 34.5 MPa 41.3 MPa 41.3 MPa
25°C 34.5 MPa 41.3 MPa 43.4 MPa
82°C 6.9 MPa 7.6 MPa 8.3 MPa
ASTM D1002. Adherends: 2024-T3 AlClad aluminum treated with chromic acid etch. Values are typical.
Effect of aluminum surface preparation
Surface preparation 7 days at 25°C 2 hours at 82°C 1 hour at 121°C
MEK wiped 26.9 MPa 29.6 MPa 38.6 MPa
Sand blasted 30.3 MPa 35.1 MPa 35.8 MPa
Wire brushed 28.2 MPa 31.0 MPa 36.5 MPa
2024-T3 AlClad aluminum; tested at 25°C after the stated cure schedule. Values are typical.
Environmental exposure performance
Exposure condition 7 days at 25°C 2 hours at 82°C 1 hour at 121°C
Control at 25°C 37.9 MPa 43.4 MPa 44.8 MPa
Water at 25°C for 30 days 25.5 MPa 30.3 MPa 30.3 MPa
100% RH at 49°C for 30 days 29.6 MPa 28.2 MPa 26.9 MPa
Anti-icing fluid for 7 days 37.9 MPa 42.7 MPa 41.3 MPa
Hydraulic oil for 7 days 38.6 MPa 44.1 MPa 45.5 MPa
JP-4 fuel for 7 days 40.0 MPa 42.0 MPa 43.4 MPa
Salt spray at 41°C for 30 days 24.1 MPa 24.1 MPa 25.5 MPa
TT-S-735 fluid for 7 days 36.5 MPa 40.7 MPa 40.0 MPa
Typical tensile lap-shear results measured at 25°C after the stated exposure and cure conditions.
Effect of bondline thickness
Bondline thickness Typical tensile lap-shear strength
0.10 mm 35.8 MPa
0.25 mm 34.5 MPa
0.51 mm 31.0 MPa
0.76 mm 31.0 MPa
1.02 mm 30.3 MPa
1.27 mm 28.2 MPa
Tested at 25°C after a 7-day cure at 25°C. Bondline thickness ranged from 0.10 to 1.27 mm.
Peel strength
Peel test 7 days at 25°C 2 hours at 82°C 1 hour at 121°C
T-peel, ASTM D1876 156 N/25 mm 205 N/25 mm 205 N/25 mm
Floating roller peel, ASTM D3167 409 N/25 mm 431 N/25 mm 471 N/25 mm
Climbing drum peel, ASTM D1781 258 m·N/m 440 m·N/m 409 m·N/m
Adherends: 2024-T3 AlClad aluminum treated with chromic acid etch. Test temperature: 25°C. Values are typical.
Next steps

Evaluate LOCTITE EA 9330 for your bonding process

Krayden can help review substrate preparation, mix and cure conditions, bondline requirements, and relevant test data for your aerospace bonding application. Contact our technical team to discuss packaging, process fit, and evaluation planning for LOCTITE EA 9330.