LOCTITE EA 9309NA

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9309NA

Main features

  • High Peel Strength on Prepared Aluminum
  • Glass, Metal, and Wood Bonding
  • 1-Hour 180 deg F Cure

Product Description

LOCTITE® EA 9309NA AERO is a two-component, toughened epoxy paste adhesive for structural bonding and repair applications. It bonds prepared metal, wood, plastic, and glass surfaces and forms flexible bonds that resist water, salt spray, and most common fluids. The adhesive is particularly notable for its peel strength on aluminum and may be cured at room temperature or with an accelerated thermal schedule. A 100:23 mix ratio by weight and a 40-minute pot life for a 450 g mass at 77°F/25°C provide a defined working window for manual application and assembly.

Key features

  • High peel strength: Delivers a typical floating-roller peel strength of 89 lbf/in (396 N/25 mm) on PAA-treated 2024-T3 Alclad aluminum under the documented test conditions.
  • Flexible, toughened bond: Provides 10% elongation at break after a 72-hour cure at 77°F/25°C, supporting applications requiring a less brittle structural adhesive.
  • Room-temperature or accelerated cure: Reaches normal performance after 3–5 days at 77°F/25°C, with 1 hour at 180°F/82°C documented as a complete accelerated cure.

Applications / Suitable for

  • Aerospace structural bonding and repair
  • Bonding prepared aluminum and other metal surfaces
  • Bonding wood and glass
  • Bonding suitable plastic surfaces

Technical Specifications

General Properties
Color
The color
Beige (Part A) / red (Part B)/ red (mixed)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:23 (by weight)
Physical Properties
Viscosity (Part B)
20–50 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured component and mixed-material properties. Component identity, temperature, test method, and mixed mass are retained where they affect interpretation.

Property Value Unit Method / condition
Product type Two-component epoxy paste adhesive — As supplied
Color Part A: beige; Part B: red; mixed: red — Visual appearance
Mix ratio, Part A:Part B 100:23 By weight Volume measurement is not recommended for structural applications unless ratio accuracy is controlled
Viscosity Part A: 150–600; Part B: 0.02–0.05; mixed: 12 Pa·s 25°C; Brookfield HBT. Part A: spindle 7 at 2.1 rad/s; Part B: spindle 1 at 10.5 rad/s; mixed: spindle 4 at 2.1 rad/s
Density Part A: 1.15; Part B: 1.00; mixed: 1.1 g/mL Uncured components and mixed adhesive
Pot life 40 minutes 450 g mass at 77°F/25°C; ASTM D2471, water bath
Shelf life 1 year Part A and Part B stored below 77°F/25°C

After-processing / final-state properties

Typical cured-material and bonded-joint results. Values apply only to the documented substrates, surface preparation, cure schedules, specimen configurations, and test conditions.

Property Value Unit Method / condition
Tensile lap shear strength 5,000 / 34.5 psi / MPa ASTM D1002; 7075-T3 Alclad aluminum, PAA per ASTM D3933; cured 3 days at 77°F/25°C; tested at 77°F/25°C
Floating-roller peel strength 89 / 396 lbf/in / N/25 mm ASTM D3167; 2024-T3 Alclad aluminum, PAA per ASTM D3933; 10 mil bondline; cured 24 hours at 77°F/25°C under 28 in-Hg; tested at 77°F/25°C
T-peel strength 46 / 205 lbf/in / N/25 mm ASTM D1876; 2024-T3 Alclad aluminum, PAA per ASTM D3933; 10 mil bondline; cured 24 hours at 77°F/25°C under 28 in-Hg; tested at 77°F/25°C
Tensile strength 4,500 / 31.0 psi / MPa ASTM D638; 0.125 in/3.18 mm casting; cured 72 hours at 77°F/25°C; tested at 77°F/25°C
Elongation at break 10 % ASTM D638; cured 72 hours at 77°F/25°C; tested at 77°F/25°C
Shore D hardness 80 Shore D ASTM D2240; cured 72 hours at 77°F/25°C; tested at 77°F/25°C
Glass-transition temperature, dry 127 / 53 °F / °C DMTA, single cantilever; cured 72 hours at 77°F/25°C; heat-up rate 5°C/min, 1 Hz, 0.1% strain
Approximate service temperature 160 / 71 °F / °C Defined as the temperature at which the adhesive retains 1,000 psi/6.9 MPa tensile lap shear strength using ASTM D1002

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers