LOCTITE EA 9309.2

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9309.2

Main features

  • 40 lb/in Peel Strength
  • 37.2 MPa Aluminum Lap Shear
  • Moderate-Viscosity Two-Part Paste

Product Description

LOCTITE EA 9309.2 is a two-part, toughened epoxy paste adhesive for metal skin, honeycomb core, and composite bonding and repair. The moderate-viscosity system offers high peel strength and develops typical aluminum tensile lap-shear values of 37.2 MPa at 25°C, 31.7 MPa at -55°C, and 6.9 MPa at 82°C. A 100:22 mix ratio by weight, 30-minute pot life for a 450 g mixed mass, and room-temperature cure support controlled structural bonding workflows. The cured material remains flexible, with 4.8% elongation at break, and resists humidity, water, and most common fluids.

Key features

  • High peel strength: Typical peel strength is 40 lb/in (178 N/25 mm) at 25°C.
  • Temperature-dependent shear performance: Typical aluminum lap shear is 31.7 MPa at -55°C, 37.2 MPa at 25°C, and 6.9 MPa at 82°C.
  • Controlled two-part mixing: Mix Part A and Part B at 100:22 by weight.
  • Practical working window: Pot life is 30 minutes for a 450 g mixed mass.
  • Flexible cured profile: Typical elongation at break is 4.8% at 25°C.

Applications / Suitable for

  • Metal skin-to-honeycomb core bonding
  • Metal and honeycomb structural repair
  • Composite bonding and repair

Technical Specifications

General Properties
Color
The color
Off white (Part A) / Blue (Part B) / Blue (Mixed)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:22 by weight
Physical Properties
Viscosity (Part A)
130,000 to 400,000 mPa.s
Viscosity (Part B)
30 to 70 mPa.s

Additional Information

Aerospace structural adhesive

LOCTITE EA 9309.2

LOCTITE EA 9309.2 is a two-part epoxy paste adhesive for metal skin, honeycomb core, and composite bonding and repair. The toughened, moderate-viscosity system combines high peel strength with aluminum lap-shear performance across low, ambient, and moderate elevated temperatures, while a 30-minute pot life for a 450 g mixed mass supports controlled application.

Two-part epoxy paste Moderate viscosity High peel strength 100:22 mix ratio by weight 30-minute pot life 5-day room-temperature cure
LOCTITE EA 9309.2 two-part aerospace structural adhesive packaging

LOCTITE EA 9309.2 two-part aerospace structural adhesive.

Before processing

As-Supplied Properties

Values describe the two-part adhesive system and its principal handling characteristics before cure.

Property Value Unit / basis Condition
Product type Two-part epoxy adhesive — Structural paste adhesive
Product form Paste — Two-part system
Consistency Moderate viscosity — As supplied
Mix ratio 100:22 Part A:Part B by weight Component mixing basis
Pot life 30 minutes 450 g mixed mass
Cure-temperature range 77–200 / 25–93 °F / °C Room-temperature through elevated-temperature cure range
Cure time 5 days Room-temperature cure
Storage temperature 82 / 28 °F / °C Product-selector handling value
Application process

Mixing and Cure

Control the component ratio, mixed quantity, and selected cure conditions when planning the bonding process.

Mix ratio: Combine Part A and Part B at 100:22 by weight.
Pot life: Plan around a 30-minute working period for a 450 g mixed mass.
Cure: The product selector lists a five-day room-temperature cure and a cure-temperature range of 77–200°F (25–93°C).
Bonded-joint evidence

Bond Strength Performance

Typical values are specific to the stated test temperature and should not be treated as universal joint-strength guarantees.

Property Value Unit Condition
Tensile lap shear at -55°C 4,600 / 31.7 psi / MPa Typical aluminum-bond result at the stated test temperature
Tensile lap shear at 25°C 5,400 / 37.2 psi / MPa Typical aluminum-bond result at the stated test temperature
Tensile lap shear at 82°C 1,000 / 6.9 psi / MPa Typical aluminum-bond result at the stated test temperature
Peel strength at 25°C 40 / 178 lb/in / N per 25 mm Typical peel result at 25°C
Service temperature 180 / 82 °F / °C Product-selector service classification
After cure

Cured Material Properties

Typical bulk-material values describe cured test specimens and are not guaranteed bonded-assembly design values.

Property Value Unit Condition
Glass transition temperature, dry 174 / 79 °F / °C Typical cured bulk property
Glass transition temperature, wet 138 / 59 °F / °C Typical cured bulk property
Tensile strength at 25°C 5,400 / 37.2 psi / MPa Typical cured bulk property
Elongation at break at 25°C 4.8 % Typical cured bulk property
Compressive strength at 25°C 7,700 / 53.0 psi / MPa Typical cured bulk property
Compressive modulus at 25°C 218 / 1,502 ksi / MPa Typical cured bulk property
Application fit

Applications

Application suitability depends on the exact substrates, surface preparation, joint design, cure profile, and service conditions.

Aerospace metal skin and honeycomb core panel prepared for structural adhesive bonding
Metal skin-to-honeycomb core bonding
The adhesive is positioned for joining metal skins and honeycomb core where a tough, permanently flexible bondline and high peel strength are important evaluation criteria.
Technician applying structural epoxy paste during metal and honeycomb repair
Metal and honeycomb repair
The moderate-viscosity, two-part paste format supports evaluation for bonded repair of metal and honeycomb structures.
Composite aerospace panel undergoing bonded structural repair
Composite bonding and repair
LOCTITE EA 9309.2 is included in the composite bonding and repair selection group, with high peel strength and a five-day room-temperature cure.
Next steps

Discuss LOCTITE EA 9309.2 for Your Bonding Process

Krayden can help review mix and cure requirements, joint geometry, service temperature, and the relevance of available shear and peel data for your metal, honeycomb, or composite bonding application.