LOCTITE EA 7000

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

LOCTITE EA 7000

Main features

  • Dual-Temperature Composite Cure
  • Extended 30-Day Out Time
  • Supported or Unsupported Film

Product Description

LOCTITE EA 7000 AERO is a modified epoxy film adhesive for composite bonding, repair and co-cure assembly. It is available in supported or unsupported constructions, with standard film weights from 0.03 to 0.10 lb/sf and thicknesses from 0.005 to 0.017 in. The green film provides dual-temperature cure capability at 121 deg C or 180 deg C and has an out time greater than 30 days at 32 deg C and 50% relative humidity. Applications include composite repair, composite surfacing, bonding pre-cured composites and co-curing with composite prepregs.

Key features

  • Supported or unsupported film: The modified epoxy film is available with or without a support construction.
  • Dual-temperature cure: The adhesive can be cured at 121 deg C or 180 deg C.
  • Extended out time: Out time is greater than 30 days at 32 deg C and 50% relative humidity.

Applications

Applications include composite repair, composite surfacing, bonding pre-cured composites and co-curing with composite prepregs.

Technical Specifications

General Properties
Color
The color
Green
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.127 - 0.38 mm
Physical Properties
Volatiles
<1 %

Additional Information

Technical properties

As-supplied properties

Supplied-film values; configuration-dependent where noted.

Property Value Unit Method / condition
ConstructionSupported or unsupportedModified epoxy film
ScrimNonwoven polyesterOther constructions available on request
Film weight0.03 to 0.10lb/sfMetric range: 146 to 488 g/m^2
Thickness0.005 to 0.017inMetric range: 0.0127 to 0.043 cm
ColorGreenAs supplied
VolatilesLess than 1%As supplied
Out timeGreater than 30daysAt 32 deg C and 50% relative humidity
Shelf lifeGreater than 2yearsAt -18 deg C