LOCTITE EA 445

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 445

Main features

  • Pre-Measured Two-Component Mixer Cup
  • 2 to 3-Minute Gel Time
  • Drillable, Tappable, Sandable Cured Epoxy

Product Description

LOCTITE® EA 445 is a two-component, room-temperature-curing epoxy adhesive supplied in a pre-measured mixer cup. It forms permanent, high-strength bonds to metals, ceramics, concrete, wood, glass, and most plastics, while also supporting repair, filling, and sealing of holes, cracks, and worn surfaces. The mixed adhesive is gray and has a gel time of 2 to 3 minutes at 25 °C. After cure, it can be drilled, tapped, sanded, machined, or painted, allowing bonded or repaired surfaces to undergo further finishing. Typical applications include production, maintenance, and prototype bonding. The product is not recommended for polyethylene or polypropylene.

Key features

  • Pre-measured two-component format: The resin and hardener are packaged in a mixer cup to support consistent proportioning and straightforward manual mixing.
  • Fast room-temperature gel: The mixed adhesive has a gel time of 2 to 3 minutes at 25 °C for rapid bonding and repair work.
  • Machinable after cure: The cured epoxy may be drilled, tapped, sanded, machined, or painted for subsequent finishing.

Applications / Suitable for

  • Production, maintenance, and prototype bonding
  • Bonding metals, ceramics, concrete, wood, glass, and most plastics
  • Repairing, filling, and sealing holes, cracks, and worn surfaces

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two-part
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
51 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1.1E16 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and curing properties for LOCTITE® EA 445 before final cure.

Property Value Method / condition
Technology Epoxy Two-component system
Resin appearance Off-white to pale gray paste As supplied
Hardener appearance Black paste As supplied
Mixed appearance Gray Uniformly mixed
Resin specific gravity 1.68 g/cm³ Typical
Hardener specific gravity 1.4 g/cm³ Typical
Gel time 2 to 3 minutes At 25 °C

After-processing / final-state properties

Typical properties of LOCTITE® EA 445 cured at 25 °C, except where otherwise noted.

Property Value Method / condition
Shore hardness 87 Shore D ISO 868
Flexural strength 55 N/mm² (7,960 psi) ASTM D790
Compressive strength 91 N/mm² (13,260 psi) ISO 604
Tensile strength 26.3 N/mm² (3,815 psi) ISO 527-2
Elongation 0.53% ISO 527-2
Thermal conductivity 0.492 W/(m·K) ASTM F433
Glass transition temperature 51 °C ASTM E1640
Coefficient of thermal expansion below Tg 39 × 10−6 K−1 ISO 11359-2
Coefficient of thermal expansion above Tg 135 × 10−6 K−1 ISO 11359-2
Volume resistivity 0.11 × 1015 ohm-cm IEC 60093
Surface resistivity 0.1 × 1015 ohms IEC 60093
Lap shear strength 13.5 N/mm² (1,955 psi) ISO 4587; grit-blasted mild steel

Leading Brands Trust in Our Products and Services