LOCTITE EA 2000

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 2000

Main features

  • Low-VOC Water-Based Nitrile-Phenolic Primer
  • Blue-to-Blue-Green Color Change
  • BMS 5-42 Type 3 Qualification

Product Description

LOCTITE EA 2000 AERO is a heat-curing, water-based nitrile-phenolic primer for anodized aluminum used with nitrile-phenolic film adhesives. The dark-blue liquid can be applied by conventional or airless spray and changes to blue-green during cure, providing a visual indication of the processed primer layer. Its low-VOC formulation contains 15 g/L VOC and is qualified to Boeing BMS 5-42, Type 3. When applied and cured under the documented conditions, the primer provides chemical and water resistance and supports metal-to-metal bonding performance across temperatures from -67°F to 250°F (-55°C to 121°C).

Key features

  • Water-based, low-VOC formulation: Contains 15 g/L VOC and uses distilled or deionized water as the thinner.
  • Visual cure indication: Changes from dark blue to blue-green when cured.
  • Aerospace qualification: Qualified to Boeing BMS 5-42, Type 3.

Applications / Suitable for

  • Priming acid-etched and phosphoric-acid-anodized aluminum
  • Use with nitrile-phenolic film adhesives
  • Spray-applied primer layers for aerospace metal bonding
Product Family

LOCTITE EA 2000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Dark blue
Solids
10–14 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
800–2500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-primer properties and storage data. Values are provided for reference and are not specification limits.

Property Value Unit Method / condition
Base Nitrile rubber, phenolic resin — As supplied
Color Dark blue — As supplied
Viscosity 800–2,500 cP Brookfield RVT, spindle #2 at 20 rpm
Weight per gallon / density 8.45 / 1.01 lb/gal / kg/L Typical
Total solids by weight 10–14 % Typical
VOC content 15 g/L Reported product feature
Calculated coverage 200 / 4.9 ft²/gal/mil / m²/L/0.0254 mm Calculated coverage
Dry time 25–45 min 1 mil wet film at 73°F (23°C) and 50% RH
Shelf life 12 months Stored at 40–60°F (4–16°C); 12 months at 50°F (10°C). Do not freeze.

After-processing / final-state properties

Mechanical results were generated on aluminum specimens prepared and tested to Boeing BMS 5-42, Class 1 requirements. The primer was applied at 0.3 mil dry-film thickness and cured for 90 minutes at 315°F (157°C). Values are typical and not specification limits.

Property Value Unit Method / condition
Cured color Blue-green — Color changes from blue during cure
Metal-to-metal lap shear 3,165 psi Tested at -67°F (-55°C)
Metal-to-metal lap shear 4,200 psi Tested at 77°F (25°C)
Metal-to-metal lap shear 1,800 psi Tested at 180°F (82°C)
Metal-to-metal lap shear 1,500 psi Tested at 250°F (121°C)
Metal-to-metal climbing peel 100 in-lb/in Tested at 77°F (25°C)

Leading Brands Trust in Our Products and Services