LOCTITE E-00CL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-00CL

Main features

  • 1:1 Two-Component Epoxy
  • 3.5-Minute Working Life
  • Electrically Insulating Epoxy

Product Description

LOCTITE® EA E-00CL™ is a fast-setting, two-component clear epoxy adhesive formulated for general-purpose structural bonding, potting, and encapsulation applications. The adhesive cures at room temperature to form a clear, rigid, machinable bond line with excellent electrical insulation properties and resistance to a wide range of chemicals and solvents. It bonds effectively to metals, plastics, glass, ceramics, rubber, and wood, making it ideal for applications where a transparent bond line is required.

Key Features & Benefits

  • Two-component clear epoxy adhesive system.
  • Fast room-temperature cure after mixing.
  • Low-viscosity formulation for easy dispensing.
  • Clear, machinable cured bond line.
  • Excellent electrical insulating characteristics.
  • Good resistance to chemicals and solvents.
  • Bonds metals, plastics, glass, wood, ceramics and rubber.

Recommended Applications

  • General-purpose industrial bonding.
  • Potting and encapsulation.
  • Electrical insulation applications.
  • Transparent bond line assemblies.
  • Plastic, metal, glass and ceramic bonding.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear (mixture)
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
7,000 - 13,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Epoxy — Two-component adhesive
Appearance (Resin) Clear to Slight Yellow — Liquid
Appearance (Hardener) Clear to Slight Yellow — Liquid
Mix Ratio (Volume) 1 : 1 Resin : Hardener By volume
Mix Ratio (Weight) 100 : 100 Resin : Hardener By weight
Resin Viscosity 7,000 - 13,000 mPa·s (cP) 25°C
Hardener Viscosity 2,200 - 4,500 mPa·s (cP) 25°C
Specific Gravity 1.1 — Resin, Hardener and Mixed
Working Life 3.5 minutes 25°C
Tack Free Time 4 minutes 25°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 20 °C Cured at 25°C
Shore Hardness 80 Shore D ISO 868
Elongation 13 % ISO 527-2
Tensile Strength 26 N/mm² ISO 527-2
Dielectric Breakdown Strength 16 kV/mm IEC 60243-1
Lap Shear Strength (Aluminum) ≥6.9 N/mm² ISO 4587, 2 h @ 65°C cure
Lap Shear Strength (Steel) 15 N/mm² 5 d @ 22°C cure
Lap Shear Strength (Stainless Steel) 13 N/mm² 5 d @ 22°C cure
Block Shear Strength (PVC) 17 N/mm² ISO 13445
Block Shear Strength (Glass) 15 N/mm² ISO 13445