Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE AA 325

Main features

  • One-Component Adhesive System
  • Rigid-Part Structural Bonding
  • Gap and Fluid Resistance

Product Description

LOCTITE® AA 325™ is a one-component, medium-viscosity structural acrylic adhesive designed for bonding close-fitting rigid metal and ceramic parts. Used with a compatible activator, the clear-to-dark-brown liquid cures at room temperature when confined between mating surfaces. Typical applications include electric-motor assemblies and other components exposed to thermal cycling, with tested resistance to automotive fluids, humidity, elevated-temperature aging, and bond gaps up to 0.5 mm under specified activator conditions.

Key features

  • Single-component application: Requires no adhesive mixing and cures with an activator at room temperature.
  • Rigid-part structural bonding: Designed for close-fitting metal and ceramic assemblies, including thermally cycled components.
  • Gap and fluid resistance: Supports bond gaps up to 0.5 mm under specified conditions and retains strength after exposure to oils, fuels, transmission fluid, coolant, and humidity.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear, dark brown liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
14,000 - 25,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Structural adhesive technology
Chemical type Modified acrylic ester — Uncured material
Appearance Clear to dark-brown liquid — TDS description; SDS confirms dark-brown liquid
Components One component — Adhesive requires no mixing
Viscosity classification Medium — TDS classification
Cure mechanism Anaerobic with activator — Cures between close-fitting parts with activator
Cure temperature Room temperature — Activator-assisted cure
Specific gravity 1.1 — At 25°C; TDS value
Dynamic viscosity 14,000–25,000 mPa·s Brookfield RVT, 25°C; spindle 6, 20 rpm
Recommended bond gap 0.1 mm TDS application guidance
Maximum stated bond gap 0.5 mm Requires activator on both surfaces and immediate assembly
Density 1.1000 g/cm³ At 20°C; current SDS value
Flash point >100 °C Tagliabue closed cup; current SDS
Auto-ignition temperature 485 °C Current SDS
Kinematic viscosity >20.5 mm²/s At 40°C; current SDS
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, activator, bond gap, cure time, temperature, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 100 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured material
Lap-shear strength 11 N/mm² Grit-blasted steel; 24-hour cure at 22°C; Activator 7075 on one side
Lap-shear strength at 0.5 mm gap ≥11 N/mm² Grit-blasted steel; 48-hour cure at 22°C; Activator 7075 on both sides
Unleaded-gasoline resistance 75 % initial strength At 87°C; 720-hour exposure; tested at 23°C
Motor-oil resistance 110 % initial strength 10W30 motor oil at 87°C; 720-hour exposure
Automatic-transmission-fluid resistance 110 % initial strength At 87°C; 720-hour exposure
Phosphate-ester resistance 110 % initial strength At 87°C; 720-hour exposure
Water/glycol resistance 75 % initial strength 50/50 water/glycol at 150°C; 720-hour exposure
Humidity resistance 75 % initial strength 100% RH at 50°C; 720-hour exposure
Heat-aging strength retention Approx. 70 % initial strength Approximately 5,000 hours at 120°C; tested at 23°C; chart-derived
Heat-aging strength retention Approx. 25 % initial strength Approximately 5,000 hours at 150°C; tested at 23°C; chart-derived