Loctite 9432 NA Epoxy Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite 9432 NA Epoxy Adhesive

Main features

Product Description

LOCTITE® EA 9432NA (also known as Hysol® Adhesive 9432NA) is an aluminum-filled, thixotropic, one-component epoxy adhesive. It is formulated to provide excellent tensile shear strength over a wide temperature range and a high degree of impact resistance. Designed to cure at moderate temperatures, it maintains a long shelf life at room temperature and can easily be pumped and dispensed without sagging.

Product Key Features

  • One-Component System - requires no mixing, simplifying application and handling.
  • Thixotropic Non-Sag Paste - dispenses easily onto parts without slumping or sagging, even on vertical surfaces.
  • Heat Cure - cures in 60 minutes at 120°C/250°F or achieves a faster cure in 30 minutes at 150°C/300°F.
  • Robust Mechanical Profile - delivers a Shore D hardness of 90, a tensile strength of 50 MPa, 1.2% elongation, and a high modulus of 4690 MPa/ 680,000 psi.
  • Excellent Resistances - provides excellent high-temperature performance and robust chemical resistance to various environmental exposures.

Applications

This adhesive fits applications requiring the bonding of a wide variety of substrates, offering exceptional tolerance to poorly prepared surfaces.

  • Metal Bonding: Bonds effectively to etched or degreased aluminum, as well as cold rolled steel, even when the steel is oily or poorly prepared.
  • Composite Assemblies: Suitable for bonding various composites, including fiberglass SMC and fiberglass vinyl ester laminates.

Technical Specifications

General Properties
Color
The color
Gray
Density
Volumetric mass per unit
1.38 kg/m3
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.38
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
1.2 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
150,000-300,000 mPa.s

Additional Information

One-Component Aluminum Filled Epoxy Adhesive

LOCTITE™ EA 9432NA

LOCTITE™ EA 9432NA (formerly known as Hysol® Adhesive 9432NA) is an aluminum-filled, thixotropic, one-component epoxy adhesive system engineered for high-performance structural bonding. Formulated to deliver outstanding tensile shear strength across a wide temperature range, this high-toughness compound provides exceptional impact resistance. It exhibits a unique tolerance for oily or poorly prepared surfaces and easily pumps or extrudes without slumping. Designed to cross-link rapidly under moderate bake temperatures, it ensures long shelf life stability and provides maximum reliability for demanding assembly workflows.

One-component (No mixing) 30 min cure at 150°C Aluminum filled paste Tolerant to oily surfaces
Contact Us

Typical engineering parameters only. Cross-linking requires a thermal activation cycle; property profiles depend on explicit baking temperatures.

LOCTITE EA 9432NA Adhesive product package
LOCTITE™ EA 9432NA

Key Features

  • Single-component formulation eliminates manual blending or volumetric tracking machinery, reducing error and scrap.
  • Thixotropic non-sag paste consistency yields clean tracking and stands up to a maximum of 0.3" slump on vertical profiles at 150°C.
  • Maintains high engineering shear strength (up to 26.2 MPa) across a wide range of hot and sub-zero environments.
  • Surface preparation tolerant, delivering robust structural bonding onto oily metals and poorly cleaned substrates.
  • Aluminum-filled epoxy grid develops superior hardness (90 Shore D) paired with maximum chemical and fluid immunity.
  • Addition cross-linking proceeded evenly throughout deep sections without generating corrosive volatile by-products.

Processing Summary

Thermal Cure Options: Curing proceeds smoothly at moderate thresholds tracking 60 minutes at 120°C. Processing cycle throughput can be accelerated to 30 minutes by raising oven environments to 150°C.
Exotherm Mitigation: Large masses of uncured compound can exotherm intensely during baking. Avoid curing static masses greater than 10 grams; thin film lines in bond areas remain completely safe.
Viscosity Rheology: Formulated as a thixotropic gray compound with a supplied viscosity scope measuring between 150,000 and 300,000 cP for reliable, easy pumping.
Contact Pressure: Parts must be held in contact and fixed continuously until full cure completes. A joint clamping pressure of 15 psi is recommended to maintain exact substrate seating.
Handling and Application Guidance

Process Notes 

Storage and Refrigeration
  • Ideally store material in cool, dry areas within unopened container vessels between 2° to 8°C (36° to 46°F).
  • Refrigerated packages must be allowed to completely return to room temperature prior to starting application cycles.
  • To avoid moisture contamination of the remaining stock, do not return any unused paste back into its original package.
Surface Preparation & Limits
  • While surface-tolerant, best bond profiles require clean, dry faces cleared of thick scaling or loose particles.
  • This epoxy grid system is not recommended for use in pure oxygen or oxygen-rich application systems.
  • Do not select or configure this compound as an industrial sealant for liquid chlorine or other strong oxidizing agents.
Clean Up & Removal
  • Uncured squeeze-out or overspray can be wiped from line components using common industrial solvents or citrus cleaners.
  • Review your fluid supplier's documentation regarding safe handling, ventilation, and flashing risks for cleaning solvents.
  • Once fully cross-linked via oven heating, this high-adhesion structural bond becomes extremely difficult to remove.
Typical Properties

Engineering Data for LOCTITE™ EA 9432NA

Physical & Cured Mechanical Characteristics

Physical Property Typical Engineering Value Test Method Standard Basis
Appearance / Color Thixotropic paste / Gray -
Viscosity 150,000 - 300,000 cP -
Specific Gravity 1.38 Measured at 77°F (25°C)
Density 1.38 g/cm3 Measured at 77°F (25°C)
Hardness 90 Shore D -
Tensile Strength 50 MPa ASTM D 638
Tensile Modulus 4690 MPa ASTM D 638
Ultimate Elongation 1.2 % ASTM D 638

Tensile Shear Strength over Varied Temperatures

Lap joints prepared with Etched Aluminum per ASTM D 1002, cured for 30 minutes at 150°C.1

Testing Ambient Temperature (°F) Typical Shear Value (MPa/psi) Thermal Performance Level
55°C (-67°F) 24 / 3,500 Cryogenic sub-zero hold stability
25°C (77°F) 26.2 / 3,800 Standard room temperature baseline validation
120°C (250°F) 20.6 / 3,000 Elevated continuous structural threshold
150°C (300°F) 16.5 / 2,400 High temperature operating limit
176.5°C (350°F ) 2.75 / 400 Extreme thermal limit values
204.5°C (400°F) 2.75 / 400 Extreme thermal limit values

Surface Tolerance & Substrate Bond Performance

Tested at 77°F per ASTM D 1002 protocols after a 30-minute cross-linking cycle at 150°C.

Substrate Matrix Profile Surface Preparation Protocol Typical Shear Strength (Mpa/psi)
Degreased Aluminum Standard chemical solvent clean 24 / 3,500
Cold Rolled Steel (Abraded) Mechanical grit abrasion + wipe 20.6 / 3,000
Cold Rolled Steel (Degreased) Solvent clean only (No abrasion) 19.6 / 2,850
Cold Rolled Steel (Oily) Untreated mill oil residue surface 18 / 2,600
Fiberglass SMC (Vinyl Ester Laminate) Standard compound surface clean 6.9 / 1,000
Fiberglass SMC (Owens Corning) Standard clean matrix boundaries 2.75 / 400 
Fiberglass SMC (Budd Co) Standard clean matrix boundaries 2.7 / 380
Environmental Fluid Resistance Profile: Lap shear joints processed on 16 gauge sandblasted cold rolled steel (5 mil bondline) maintain robust load values at 25°C (77°F) following a complete 30-day continuous immersion soak across automotive chemicals including water, 10W40 motor oil, 50% ethylene glycol (ambient and boiling lines), brake fluid, automatic transmission fluid, gasoline, and diesel fuel.
LOCTITE® EA 9432NA Strength Developments at various temperatures 

Applications

Where LOCTITE™ EA 9432NA Fits

Automotive sheet steel panel stamping assembly loop
Contaminated Substrate Joints
Perfectly optimized for industrial processing areas where strict mechanical surface abrasion or heavy solvent degreasing is impossible or impractical.
  • Cures reliably straight through protective mill oil residues.
  • Maintains high structural shear thresholds (2,600 psi) on oily steel.
  • Bypasses extensive chemical surface conditioning line pre-steps.
High temperature industrial electronics structural assembly
Extreme Thermal Operating Zones
Engineered to deliver heavy mechanical structural load holding capacities when exposed to sustained thermal environments up to 150°C (300°F).
  • Retains an impressive 2,400 psi shear capacity at 150°C (300°F).
  • Resists physical degradation under prolonged hot air aging.
  • Maintains stable mechanical strength under severe thermal shock cycles.
Vertical structural seam assembly dispensing epoxy paste
Vertical & Overhead Seams
High thixotropic paste rheology makes this adhesive highly dispensable via automatic pump systems while remaining non-sag on perpendicular joint faces.
  • Easily pumped and dispensed onto complex parts.
  • Bead tracking stays completely immune to running risks.
  • Limits gravity slump to a tight 0.3" maximum during heat bakes.
Package & Support

Standard Packaging & Technical Help

Standard Packaging
  • Supplied ready-to-use inside standard industrial packaging and cartridge configurations.
  • Single-component paste system requires no automated static or dynamic nozzle mixing valves.
  • Original containers preserve long-term product shelf life stability under cold storage control.
Technical Help Capabilities
  • Designing optimized thermal profiles to enable accelerated 30-minute high-temperature bonding lines.
  • Auditing custom part geometries and line setups to safely isolate and manage exothermic mass reactions.
  • Configuring high-pressure pump feed parameters matching specified compound viscosities (150k-300k cP).
  • Support for localized test coupon trials to verify target cohesive failure lap shear limits.
Technical Guidance

Tips and Troubleshooting

Issue Recommended Action
Material demonstrates excessive joint squeeze-out or gravity slump inside the heating oven
  • Ensure total batch stock returns fully to ambient room temperature before triggering extrusion cycles.
  • Verify that the assembly line clamping fixtures maintain a steady, uniform pressure profile of 15 psi.
  • Monitor localized heating limits; check that vertical slump parameters remain under the 0.3" max threshold at 150°C (300°F).
Material mass chars, bubbles, or alters substrate shape during high-temperature bakes
  • Large pocket accumulations of uncured adhesive generate intense exothermic energy during cross-linking.
  • Avoid placing or leaving localized compound masses larger than 10 grams inside static configurations.
  • Ensure joint designs employ proper structural film tracking; thin paste layers within bond lines are completely safe.
  • Do not program thermal activation cycles exceeding the maximum recommended threshold of 350°F.
Adhesion tracking breakdown or low lap shear force values over difficult plastics
  • While surface-tolerant on oily metals, unprimed structural bonds will not stick onto Teflon, PE, or PP.
  • Clear thick boundary layer greases or contaminants using industrial solvents; avoid acetone/IPA alone for heavy oils.
  • Introduce localized fine mechanical surface abrasion, chemical etching, plasma exposure, or specialized primers.
  • Screen rubber or plastic parts for high plasticizer loading; mobile plasticizers act as active bond release agents.
Next Steps

Ready to Qualify LOCTITE™ EA 9432NA?

Tell us about your performance, design, and manufacturing challenges. Share your specific substrate pairings, joint geometry designs, takt time constraints, and environmental testing parameters. Our global technical support team is prepared to put our industrial adhesive expertise and process knowledge to work for your production floor.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers