LOCTITE 8060

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 8060 LOCTITE 8060

Main features

  • High-Temperature Anti-Seize Protection
  • Controlled Stick Application
  • Measured Assembly Torque Behavior

Product Description

LOCTITE LB 8060 is a silver, non-curing anti-seize lubricant supplied as an application stick for threaded and closely fitted metal parts. The naphthenic-oil formulation supports controlled placement on fine threads, snug slip fits, boiler and oven components, jet-engine hardware, and industrial turbines within the product's service limits. Typical use extends to 870 deg C, and the torque coefficient is 0.18 on 3/8 x 16 steel nuts and bolts. It is not a high-speed load-carrying lubricant and must not be used on ball or roller bearings or parts where lubrication is critical.

Key features

  • High-temperature anti-seize protection: Typical use reaches up to 870 deg C for threaded and closely fitted metal assemblies.
  • Controlled stick application: The solid format supports direct placement without dispensing a loose paste.
  • Measured assembly torque behavior: A torque coefficient of 0.18 is reported on 3/8 x 16 steel nuts and bolts.

Applications / Suitable for

  • Anti-seize protection for fine threads
  • Snug slip fits and closely mated metal parts
  • High-temperature boiler, oven, turbine, and jet-engine hardware within listed limits

Technical Specifications

General Properties
Chemistry Type
Naphthenic oil
Color
The color
Silver color/ Stick
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One component
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Chemical Properties
Copper Corrosion
Slight tarnish, 1a

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values and characteristics for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceSilver-As supplied
Product formStick-As supplied
Base fluidNaphthenic oil-Formulation description
Cure behaviorNon-curing-As supplied and in service
Specific gravity1.1-25 deg C
Penetration20 to 800.1 mmISO 2137
Technical properties

After-processing / final-state properties

Typical values for the cured, bonded, treated, or in-service product under the listed conditions.

PropertyValueUnitMethod / condition
Typical use temperatureUp to 870deg CTypical use guidance
Torque coefficient0.18-3/8 x 16 steel nuts and bolts
Copper corrosion rating1a, slight tarnish-ISO 2160
Dimensional stabilityPass-77 deg C

Leading Brands Trust in Our Products and Services