LOCTITE 680

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 680

Main features

  • High-Strength Cylindrical Retention
  • Gap-Filling Cylindrical Retention
  • Heat and Fluid Resistance

Product Description

LOCTITE® 680™ is a one-component, high-strength anaerobic retaining compound designed for bonding close-fitting cylindrical metal parts where medium viscosity is preferred. The green methacrylate ester liquid cures when confined between mating metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. It delivers robust curing on active metals such as mild steel and passive substrates including stainless steel and plated surfaces, while tolerating minor contamination from cutting, lubricating, anti-corrosion, and protective oils.

Key features

  • High-strength retention: Develops up to 28 N/mm² compressive shear strength on stainless-steel pins and collars after a seven-day cure.
  • Gap-filling cylindrical bonding: Supports close-fitting metal assemblies and maintains useful strength across tested gaps from 0.05 to 0.25 mm.
  • Heat and fluid resistance: Retains strength after exposure to motor oil, gasoline, brake fluid, water/glycol, ethanol, acetone, biodiesel, and diesel exhaust fluid.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
750 - 1,750 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Green liquid — Uncured material
Fluorescence Positive under UV light — Inspection aid
Components One component — No mixing required
Viscosity classification Medium — Retaining application
Cure mechanism Anaerobic — Cures when confined between close-fitting metal surfaces without air
Secondary cure Activator — May accelerate cure or support larger gaps
Strength classification High — Cylindrical retaining application
Specific gravity 1.1 — At 25°C; TDS value
Dynamic viscosity 750–1,750 mPa·s Brookfield RVT, 25°C; spindle 3, 20 rpm
Dynamic viscosity 650–1,850 mPa·s Cone and plate, 25°C; shear rate 129 s−1
Dynamic viscosity 450–550 mPa·s SDS value; method not stated
Density 1.1 g/cm³ At 20°C; SDS value
Flash point >100 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, bond gap, temperature, activator use, cure time, surface condition, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 52 × 10−6 K−1 ISO 11359-2
Compressive shear strength ≥24.1 N/mm² ISO 10123; steel pins and collars; cured 1 hour at 93°C and tested at 22°C
Compressive shear strength ≥19.3 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 22°C
Compressive shear strength 26 N/mm² ISO 10123; steel pins and collars; cured 7 days at 22°C
Compressive shear strength 28 N/mm² ISO 10123; stainless-steel pins and collars; cured 7 days at 22°C
Compressive shear strength 16 N/mm² ISO 10123; aluminum pins and collars; cured 7 days at 22°C
Breakaway torque 35 N·m ISO 10964; M10 black-oxide bolts and mild-steel nuts; cured 24 hours at 22°C
Prevail torque 28 N·m ISO 10964; M10 black-oxide bolts and mild-steel nuts; cured 24 hours at 22°C
Motor-oil resistance 145 % initial strength 5W40 synthetic motor oil at 125°C; 1,000-hour exposure
Unleaded-gasoline resistance 110 % initial strength At 22°C; 1,000-hour exposure
Brake-fluid resistance 110 % initial strength At 22°C; 1,000-hour exposure
Water/glycol resistance 135 % initial strength 50/50 water/glycol at 87°C; 1,000-hour exposure
Ethanol resistance 100 % initial strength At 22°C; 1,000-hour exposure
Acetone resistance 100 % initial strength At 22°C; 1,000-hour exposure
B100 biodiesel resistance 110 % initial strength At 22°C; 1,000-hour exposure
DEF resistance 110 % initial strength AdBlue-type diesel exhaust fluid at 22°C; 1,000-hour exposure
E85 ethanol-fuel resistance 105 % initial strength At 22°C; 1,000-hour exposure