LOCTITE 648

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE 648

Main features

  • High-Strength Cylindrical Retention
  • Metal Compatibility Cylindrical Retention
  • Heat, Oil, and Contamination Resistance

Product Description

LOCTITE® 648™ is a one-component, high-strength anaerobic retaining compound designed for bonding close-fitting cylindrical metal parts, particularly assemblies with bond gaps approaching 0.15 mm. The low-viscosity green urethane methacrylate liquid cures when confined between mating metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. It performs on active and passive metals, tolerates minor surface contamination from industrial oils, and is commonly used to retain gears and sprockets on gearbox shafts and rotors on electric-motor shafts.

Key features

  • High-strength cylindrical retention: Develops up to 31 N/mm² compressive shear strength on steel pins and collars after a 72-hour cure.
  • Broad metal compatibility: Works on active metals such as mild steel and passive substrates including stainless steel and plated surfaces.
  • Heat, oil, and contamination tolerance: Supports elevated-temperature applications and tolerates minor contamination from cutting, lubricating, anti-corrosion, and protective fluids.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Urethane methacrylate — Uncured material
Appearance Green liquid — Uncured material
Fluorescence Positive under UV light — Inspection aid
Components One component — No mixing required
Viscosity classification Low — Retaining application
Cure mechanism Anaerobic — Cures when confined between close-fitting metal surfaces without air
Secondary cure Activator — May accelerate cure on passive metals or in larger gaps
Strength classification High — Cylindrical retaining application
Specific gravity 1.1 — At 23°C; TDS value
Dynamic viscosity 500 mPa·s Brookfield RVT, 25°C; spindle 2, 20 rpm
Dynamic viscosity 500 mPa·s Cone and plate, 25°C; shear rate 129 s−1
Dynamic viscosity range 450–550 mPa·s SDS value; method not stated
Density 1.1 g/cm³ At 20°C; SDS value
Flash point >100 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, bond gap, temperature, activator use, cure time, surface condition, and test method.

Property Value Unit Method / condition
Glass-transition temperature 100 °C ISO 11359-2; cured 24 hours at 23°C
Coefficient of thermal expansion below Tg 93 × 10−6 K−1 ISO 11359-2
Coefficient of thermal expansion above Tg 184 × 10−6 K−1 ISO 11359-2
Compressive shear strength 13.5 N/mm² ISO 10123; steel pins and collars; cured 15 minutes at 23°C
Compressive shear strength 31 N/mm² ISO 10123; steel pins and collars; cured 72 hours at 23°C
Compressive shear strength 30 N/mm² ISO 10123; stainless-steel pins and collars; cured 72 hours at 23°C
Compressive shear strength 18 N/mm² ISO 10123; aluminum pins and collars; cured 72 hours at 23°C
Breakaway torque 58 N·m ISO 10964; M10 black-oxide bolts and mild-steel nuts; cured 72 hours at 23°C
Prevail torque 40 N·m ISO 10964; M10 black-oxide bolts and mild-steel nuts; cured 72 hours at 23°C
Motor-oil resistance 145 % initial strength 5W40 synthetic motor oil at 125°C; 5,000-hour exposure
Unleaded-petrol resistance 105 % initial strength At 23°C; 5,000-hour exposure
Brake-fluid resistance 125 % initial strength At 23°C; 5,000-hour exposure
Water/glycol resistance 80 % initial strength 50/50 water/glycol at 87°C; 5,000-hour exposure
Ethanol resistance 120 % initial strength At 23°C; 5,000-hour exposure
Acetone resistance 100 % initial strength At 23°C; 5,000-hour exposure
B100 biodiesel resistance 100 % initial strength At 23°C; 5,000-hour exposure
DEF resistance 100 % initial strength AdBlue-type diesel exhaust fluid at 23°C; 5,000-hour exposure