LOCTITE 620

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 620

Main features

  • High Temperature Retention
  • Gap-Filling Cylindrical Retention
  • High Mechanical and Fluid Resistance

Product Description

LOCTITE® 620™ is a one-component, high-viscosity anaerobic retaining compound designed for bonding cylindrical metal parts, particularly assemblies with bond gaps approaching 0.2 mm and applications requiring robust elevated-temperature performance. The green methacrylate ester liquid cures when confined between close-fitting metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. Typical applications include retaining locating pins in radiator assemblies, securing bearings in automotive transmissions, and locking bushings and sleeves into housings or onto shafts.

Key features

  • High-temperature cylindrical retention: Designed for demanding retaining applications where elevated-temperature performance is required.
  • Gap-filling capability: Supports cylindrical assemblies with bond gaps approaching 0.2 mm.
  • Robust mechanical and fluid resistance: Develops high compressive shear strength and retains performance after prolonged exposure to oils, fuels, brake fluid, water/glycol, ethanol, and acetone.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.16
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
8,500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Green liquid — Uncured material
Components One component — No mixing required
Viscosity classification High — Retaining application
Cure mechanism Anaerobic — Cures when confined between close-fitting metal surfaces without air
Secondary cure Activator — May accelerate cure or support larger gaps and inactive surfaces
Strength classification Medium to high — Cylindrical retaining application
Specific gravity 1.16 — At 23°C; TDS value
Dynamic viscosity 8,500 mPa·s Brookfield RVT, 25°C; spindle 5, 20 rpm
Viscosity 1,800 mPa·s EN 12092-MV, 25°C; after 180 seconds, shear rate 129 s−1
Density 1.16 g/cm³ At 20°C; SDS value
Flash point >100 °C SDS value
Auto-ignition temperature >300 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, bond gap, temperature, activator use, cure schedule, surface preparation, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 80 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Elongation at break <1 % ISO 37
Compressive shear strength 17 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 23°C
Compressive shear strength after heat cure 24 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 23°C plus 24 hours at 177°C; tested at 23°C
Motor-oil resistance 100 % initial strength At 125°C; 1,000-hour exposure
Unleaded-petrol resistance 95 % initial strength At 22°C; 1,000-hour exposure
Brake-fluid resistance 100 % initial strength At 22°C; 1,000-hour exposure
Water/glycol resistance 80 % initial strength 50/50 water/glycol at 87°C; 1,000-hour exposure
Ethanol resistance 75 % initial strength At 22°C; 1,000-hour exposure
Acetone resistance 95 % initial strength At 22°C; 1,000-hour exposure

Leading Brands Trust in Our Products and Services