LOCTITE 609

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE 609

Main features

  • High-Strength Cylindrical Retention
  • Low-Viscosity Retention Application
  • Vibration and Fluid Resistance

Product Description

LOCTITE® 609™ is a one-component, high-strength anaerobic retaining compound designed for bonding close-fitting cylindrical metal parts. The low-viscosity green methacrylate ester liquid cures when confined between mating metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. Typical applications include securing bushings and sleeves in housings or on shafts, bonding rotor assemblies, and augmenting press, slip, and shrink fits.

Key features

  • High-strength cylindrical retention: Develops compressive shear strength of at least 15.8 N/mm² on steel pins and collars after 24 hours.
  • Low-viscosity gap penetration: Supports close-fitting slip, press, and shrink-fit assemblies with controlled bond gaps.
  • Vibration and fluid resistance: Helps prevent movement and leakage while retaining strength after exposure to oils, fuels, brake fluid, ethanol, and water/glycol.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
110 - 140 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Green liquid — Uncured material
Fluorescence Positive under UV light — Inspection aid
Components One component — No mixing required
Viscosity classification Low — Retaining application
Cure mechanism Anaerobic — Cures when confined between close-fitting metal surfaces without air
Secondary cure Activator — May improve cure speed on inactive surfaces or larger gaps
Strength classification High — Cylindrical retaining application
Specific gravity 1.1 — At 25°C; TDS value
Viscosity 110–140 mPa·s Cannon-Fenske, ISO 3104
Density 1.1 g/cm³ At 20°C; SDS value
Flash point >100 °C Tagliabue closed cup; SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on substrate, bond gap, temperature, activator use, cure time, surface condition, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 80 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Elongation at break <2 % ISO 37
Compressive shear strength ≥10.3 N/mm² ISO 10123; steel pins and collars; cured 1 hour at 22°C
Compressive shear strength ≥15.8 N/mm² ISO 10123; steel pins and collars; cured 24 hours at 22°C
Motor-oil resistance 100 % initial strength MIL-L-46152 motor oil at 125°C; 1,000-hour exposure
Unleaded-gasoline resistance 100 % initial strength At 22°C; 1,000-hour exposure
Brake-fluid resistance 100 % initial strength At 22°C; 1,000-hour exposure
Water/glycol resistance 80 % initial strength 50/50 water/glycol at 87°C; 1,000-hour exposure
Ethanol resistance 100 % initial strength At 22°C; 1,000-hour exposure
Acetone resistance 85 % initial strength At 22°C; 1,000-hour exposure