LOCTITE 569

Main features

  • Low-Viscosity Sealing Application
  • Vibration-Resistant Thread Sealing
  • Broad Fluid Resistance

Product Description

LOCTITE® 569™ is a one-component, low-viscosity anaerobic thread sealant designed for locking and sealing close-fitting metal pipes and fittings. The brown methacrylate ester liquid cures when confined between mating metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. Its low-strength formulation supports service disassembly, while its fluid resistance makes it suitable for industrial threaded connections exposed to oils, fuels, water, transmission fluid, brake fluid, and phosphate-ester fluids.

Key features

  • Low-viscosity thread sealing: Flows into close-fitting metal threads to support complete coverage of the threaded interface.
  • Vibration-resistant locking: Helps prevent threaded fittings from loosening or leaking under shock and vibration.
  • Broad fluid resistance: Retains performance after extended exposure to common industrial oils, fuels, water, and hydraulic fluids.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Brown liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
300 - 500 mPa.s
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.1 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Brown liquid — Uncured material
Fluorescence Negative — Uncured material
Components One component — No mixing required
Strength classification Low — Thread-sealing application
Specific gravity 1.05 — At 25°C
Viscosity 300–500 mPa·s Cannon-Fenske, ISO 3104
Density 1.049 g/cm³ At 20°C; SDS value
Flash point >100 °C Tagliabue closed cup; SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, assembly geometry, surface condition, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 0.1 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Breakaway torque ≥2.8 N·m ISO 10964; degreased 3/8 × 24 grade-2 steel nuts and bolts; cured 24 hours at 22°C
Prevail torque ≥1.1 N·m ISO 10964; degreased 3/8 × 24 grade-2 steel nuts and bolts; cured 24 hours at 22°C
Breakaway torque after 1 hour ≥1.1 N·m ISO 10964; degreased 3/8 × 24 grade-2 steel nuts and bolts; 22°C
Prevail torque after 1 hour ≥0.6 N·m ISO 10964; degreased 3/8 × 24 grade-2 steel nuts and bolts; 22°C
Motor-oil resistance 100 % initial strength MIL-L-46152 motor oil at 87°C; 720-hour exposure
Unleaded-gasoline resistance 100 % initial strength At 87°C; 720-hour exposure
Phosphate-ester resistance 100 % initial strength At 87°C; 720-hour exposure
Brake-fluid resistance 78 % initial strength At 87°C; 720-hour exposure