LOCTITE 567

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 567

Main features

  • High-Lubricity Thread Assembly
  • Anaerobic Thread Sealing
  • High-Temperature Service Sealant Formulation

Product Description

LOCTITE® 567™ is a one-component, low-strength anaerobic thread sealant designed for locking and sealing tapered metal pipes and fittings. The smooth, creamy off-white methacrylate ester paste cures when confined between close-fitting metal surfaces in the absence of air, helping prevent loosening and leakage caused by shock and vibration. Its high lubricity helps reduce galling during assembly, while robust cure performance, elevated-temperature capability, and oil tolerance support demanding industrial fluid-power and process applications.

Key features

  • High-lubricity thread sealing: Helps prevent galling on stainless steel, aluminum, and other metal pipe threads and fittings.
  • Robust anaerobic cure: Cures on active and passive metal surfaces and tolerates minor contamination from common industrial oils.
  • High-temperature service: Supports demanding metal-thread applications with resistance to elevated temperatures and a range of industrial fluids.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Smooth, creamy, off-white paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
540,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Methacrylate ester — Uncured material
Appearance Smooth, creamy, off-white paste — Uncured material
Components One component — No mixing required
Strength classification Low — Thread-sealing application
Specific gravity 1.1 — At 23°C
Viscosity 540,000 mPa·s Brookfield RVF, 25°C; spindle 7, 2 rpm
Density 1.15 g/mL At 20°C; SDS value
Flash point 100 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on the stated cure schedule, substrate, temperature, activator use, assembly geometry, and test method.

Property Value Unit Method / condition
Breakaway torque 12 N·m ISO 10964; unseated M10 black-oxide bolts and mild-steel nuts
Breakaway torque 12 N·m ISO 10964; unseated M10 brass bolts and nuts
Breakaway torque 8.0 N·m ISO 10964; unseated M10 stainless-steel bolts and nuts
Breakloose torque 17 N·m ISO 10964; M10 black-oxide bolts and steel nuts, pre-torqued to 5 N·m
Removal torque 50 N·m ASTM D6396; 3/8 NPT steel pipes and plugs, cured 24 hours at 22°C, pre-torqued to 27 N·m
Cold-strength test limit −75 °C Product tested to this temperature
Motor-oil resistance 100 % initial strength MIL-L-46152 motor oil at 125°C; 1,000-hour exposure
Water/glycol resistance 95 % initial strength 50/50 water/glycol at 87°C; 1,000-hour exposure
B100 biodiesel resistance 105 % initial strength At 22°C; 1,000-hour exposure
DEF resistance 120 % initial strength AdBlue®/DEF at 22°C; 1,000-hour exposure

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers