LOCTITE 435

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 435 LOCTITE 435

Main features

  • Rubber-Toughened Peel Resistance
  • Low-Viscosity Rapid Bonding
  • Porous-Material Bonding Range

Product Description

LOCTITE 435 is a one-part, low-viscosity, rubber-toughened ethyl cyanoacrylate instant adhesive for metals, plastics, rubbers, and selected porous materials. The toughened formulation combines increased flexibility and peel strength with resistance to shock. A viscosity of 100 to 250 mPa s supports rapid wetting and thin bondlines, while fixture time ranges from under 5 seconds on nitrile rubber and balsa wood to 30 to 60 seconds on common metal substrates. The adhesive also bonds wood, paper, leather, and fabric when those materials fit the assembly requirements.

Key features

  • Rubber-toughened flexibility: The cured adhesive provides increased flexibility and peel strength with enhanced shock resistance.
  • Low-viscosity rapid wetting: A 100 to 250 mPa s viscosity supports thin bondlines and fast fixture on many substrates.
  • Porous-material bonding range: The product supports selected wood, paper, leather, and fabric assemblies in addition to common engineering materials.

Applications / Suitable for

  • Shock- and peel-resistant bonding of metals
  • Bonding plastics, rubbers, and elastomers
  • Bonding selected porous or absorbent materials

Technical Specifications

General Properties
Chemistry Type
Ethyl cyanoacrylate with
Color
The color
Colorless to straw colored, slightly cloudy liquid
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One component
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
130 °C
Linear thermal expansion
80x10^-6 K-1
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.1 W/m.K
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100 to 250 mPa.s
Mechanical Properties
Peel Strength
4 N/mm
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
25 kV/mm
Surface Resistivity
10×10^15 Ohms Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10×10^15 Ohms⋅cm
Curing Conditions
Fixture Time
30 to 45 seconds

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure, application, or assembly.

PropertyValueUnitMethod / condition
AppearanceColorless to straw, slightly cloudy liquid-Uncured
Chemical typeEthyl cyanoacrylate-As supplied
ComponentsOne part-No mixing required
Specific gravity1.1-25 deg C
Viscosity100 to 250mPa sCone and plate, 25 deg C, shear rate 1,000 s^-1
Cure mechanismHumidity-Atmospheric moisture
Technical properties

After-processing / final-state properties

Typical values for the cured or installed product under the listed conditions.

PropertyValueUnitMethod / condition
Fixture time, nitrile rubber<5s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, ABS10 to 20s22 deg C, 50% RH; time to 0.1 N/mm^2 shear strength
Fixture time, aluminum<=60sIsopropanol-wiped aluminum, 22 deg C, 50% RH
Glass transition temperature130deg CISO 11359-2; cured 24 h at 22 deg C
Lap shear strength, grit-blasted steel19N/mm^2Cured 24 h at 22 deg C
180-degree peel strength, grit-blasted steel4N/mmISO 8510-2; cured 48 h at 22 deg C
Side impact resistance, aluminum>=4JCured 24 h at 22 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers