LOCTITE 4306

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 4306

Main features

  • Dual-Cure Bonding Processing
  • Low-Blooming Bonding Cure
  • Rapid Surface and Fixture Curing

Product Description

LOCTITE® 4306™ is a one-component UV/light-curing cyanoacrylate adhesive formulated with a photoinitiator to provide ultra-fast fixture speeds, surface cure and fillet cure capabilities. The adhesive combines UV/visible light curing with a secondary moisture-cure mechanism, enabling reliable bonding of plastics, rubbers and metals while minimizing blooming. Its fluorescent properties under UV light allow easy inspection of adhesive presence and coverage. LOCTITE 4306 has been tested to Henkel protocols based on ISO 10993 biocompatibility standards and is widely used in the assembly of disposable medical devices and precision components requiring rapid processing and inspection.

Key Features & Benefits

  • Dual-cure technology combining UV/visible light cure with secondary humidity cure.
  • Very rapid surface and fixture curing performance.
  • Fluoresces under UV light for inspection and quality control.
  • Low blooming characteristics compared with conventional cyanoacrylates.
  • One-component adhesive requiring no mixing.
  • Suitable for plastics, rubbers and metal substrates.
  • Evaluated using ISO 10993-based biocompatibility protocols for medical device applications.

Recommended Applications

  • Disposable medical device assembly.
  • UV-curable bonding processes requiring rapid fixture speed.
  • Plastic, rubber and metal component assembly.
  • Applications requiring fluorescent bond-line inspection.
  • Precision manufacturing and automated assembly systems.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent, light yellow-green to dark blue-green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
10 - 35 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate / UV — Ethyl cyanoacrylate with photoinitiator
Chemical Type Ethyl Cyanoacrylate — UV/light-curable formulation
Appearance Transparent Light Yellow-Green to Dark Blue-Green Liquid — Uncured
Fluorescence Positive Under UV Light — Inspection capability
Components One Part — No mixing required
Specific Gravity 1.05 — 25°C
Viscosity 10 - 35 mPa·s (cP) Cone & Plate, 3,000 s⁻¹, 25°C
Primary Cure UV / Visible Light — Light activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 116 °C ASTM E228
Coefficient of Thermal Expansion (Pre Tg) 92 × 10⁻⁶ K⁻¹ ISO 11359-2
Shore Hardness 82 Shore D ISO 868
Tensile Strength 32.5 N/mm² ISO 527-3
Tensile Modulus 1,730 N/mm² ISO 527-3
Elongation at Break 2.2 % ISO 527-3
Volume Shrinkage 16 % ASTM D792
Water Absorption (7 Days @ 22°C) 1.1 % ISO 62
Block Shear Strength (Polycarbonate) ≥9.0 N/mm² ISO 13445, UV Cured
Block Shear Strength (Polycarbonate to Polycarbonate) 15.2 N/mm² UV Cure @ 365 nm