LOCTITE 426

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE 426

Main features

  • Toughened Structural Bonding
  • Impact-Resistant Cyanoacrylate Bonding
  • Gel-Consistency Bonding Placement

Product Description

LOCTITE® 426 is a one-component, black ethyl cyanoacrylate adhesive gel toughened with elastomers to provide enhanced impact resistance, peel strength and durability. The adhesive is specifically formulated to improve resistance to heat and humidity while maintaining the rapid curing characteristics of cyanoacrylate technology. Designed for bonding metals, plastics and rubbers, LOCTITE 426 offers controlled application due to its gel consistency, making it suitable for vertical surfaces and applications requiring precise adhesive placement. The product cures through exposure to ambient humidity and develops strong structural bonds with excellent environmental resistance.

Key Features & Benefits

  • Elastomer-toughened cyanoacrylate gel formulation.
  • High impact and peel strength performance.
  • Improved heat and humidity resistance.
  • One-component adhesive requiring no mixing.
  • Fast humidity-activated curing mechanism.
  • Bonds metals, plastics and rubbers effectively.
  • Gel consistency minimizes running and migration.

Recommended Applications

  • Impact-resistant industrial assemblies.
  • Metal, plastic and rubber bonding.
  • Applications exposed to heat and humidity.
  • Maintenance and repair operations.
  • Vertical and controlled-placement bonding applications.
Product Family

LOCTITE 426

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black liquid
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
7,000 - 14,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Elastomer-toughened ethyl cyanoacrylate gel
Chemical Type Ethyl Cyanoacrylate — Impact-resistant adhesive
Appearance Black Liquid Gel — Uncured
Components One Part — No mixing required
Viscosity 7,000 - 14,000 mPa·s (cP) Brookfield HBT, Spindle 3, 20 rpm, 25°C
Cure Mechanism Humidity Cure — Activated by atmospheric moisture
Key Substrates Metals, Plastics and Rubbers — General-purpose bonding
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Impact Resistance Enhanced — Elastomer toughened formulation
Peel Strength Enhanced — Improved peel performance
Heat Resistance Improved — Compared with standard cyanoacrylates
Humidity Resistance Improved — Enhanced environmental durability
Lap Shear Strength (Steel) ≥16.5 N/mm² ISO 4587, 48 h Cure @ 22°C
Lap Shear Strength (Steel, Tested at 121°C) ≥4.8 N/mm² After 24 h @ 22°C + 24 h @ 121°C
Lap Shear Strength (Steel After Heat Exposure) ≥20.7 N/mm² Tested @ 22°C after 24 h @ 121°C
Cure Type Moisture Activated — Cyanoacrylate polymerization