LOCTITE 422

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 422

Main features

  • High-Viscosity Cyanoacrylate Gel
  • Transparent Cured Bondline
  • Documented MIL-A-46050C/A-A-3097 Qualification

Product Description

LOCTITE® 416™ is a one-component, high-viscosity ethyl cyanoacrylate instant adhesive formulated for general-purpose bonding of plastics, rubbers and metals. The transparent adhesive delivers rapid fixture times through moisture-activated curing and develops high bond strength on a wide range of substrates. Its higher viscosity enables better control during application while maintaining the fast-curing performance expected from cyanoacrylate technology. LOCTITE 416 also meets the lot requirements of Military Specification Mil-A-46050C and is qualified to Commercial Item Description A-A-3097, making it suitable for industrial assembly, maintenance and repair applications.

Key Features & Benefits

  • High-viscosity ethyl cyanoacrylate formulation.
  • One-component adhesive requiring no mixing.
  • Fast humidity-activated room-temperature cure.
  • Bonds plastics, rubbers and metals effectively.
  • Transparent cured bondline appearance.
  • Qualified to Mil-A-46050C and A-A-3097 specifications.
  • Excellent chemical and environmental resistance after cure.

Recommended Applications

  • General-purpose industrial bonding.
  • Plastic and rubber component assembly.
  • Metal-to-metal and mixed-material bonding.
  • Maintenance and repair operations.
  • High-strength precision assembly applications.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Clear liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.05
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,000 - 2,500 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Ethyl cyanoacrylate adhesive
Chemical Type Ethyl Cyanoacrylate — General purpose instant adhesive
Appearance Transparent Clear Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.05 — 25°C
Viscosity (Cone & Plate) 900 - 1,500 mPa·s (cP) 100 s⁻¹, 25°C
Brookfield Viscosity 1,150 - 1,500 mPa·s (cP) LVF, Spindle 2, 12 rpm
Key Substrates Plastics, Rubbers and Metals — Typical bonding applications
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Coefficient of Thermal Expansion 100 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/m·K ISO 8302
Softening Point 165 °C DIN EN 1427
Volume Resistivity 2 × 10¹⁵ to 10 × 10¹⁵ Ω·cm IEC 60093
Surface Resistivity 10 × 10¹⁵ to 80 × 10¹⁵ Ω IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Lap Shear Strength (Steel) 18 - 26 N/mm² ISO 4587, Grit Blasted Steel
Lap Shear Strength (Aluminum) 12 - 19 N/mm² ISO 4587, Etched Aluminum
Tensile Strength (Steel) 12 - 25 N/mm² ISO 6922
Tensile Strength (Buna‑N) ≥6.0 N/mm² ISO 6922, 10 s Cure @ 22°C
T-Peel Strength (Steel) <0.5 N/mm ISO 11339

Leading Brands Trust in Our Products and Services