LOCTITE 4047

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE 4047

Main features

  • Rapid Blue-or-UV Photocure
  • High-Viscosity Placement Control
  • Low-Shrink Mechanical Stability

Product Description

LOCTITE ECCOBOND LUX 4047 is a single-component, high-viscosity acrylate adhesive and encapsulant for photocured optoelectronic assembly. The opaque yellowish-white material cures in seconds with suitable visible blue or UV light and combines low cure shrinkage with high mechanical stability. A viscosity of 120,000 mPa s supports controlled placement. The cured material has Shore D 80 hardness, 1.1% linear shrinkage, and 0.07% water absorption after 24-hour immersion. It is used for fiber-optic and optoelectronic device assembly, including LED mounting, laser-diode packaging, fiber pigtailing, and transceiver potting.

Key features

  • Rapid Blue-or-UV Photocure: The adhesive cures in seconds under suitable visible blue or UV light.
  • High-Viscosity Placement: A 120,000 mPa s viscosity supports controlled placement in optoelectronic assemblies.
  • Low-Shrink Stable Cure: The cured material combines 1.1% linear shrinkage with Shore D 80 hardness.

Applications / Suitable for

  • Fiber-optic and optoelectronic device assembly
  • LED mounting and laser-diode packaging
  • Fiber pigtailing and transceiver potting
Product Family

LOCTITE 4047

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Opaque yellowish white
Chemistry Type
UV acrylic
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
One component
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
52 °C
Physical Properties
Tack-Free Time
>60 minutes
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
120,000 mPa.s
Chemical Properties
Water Absorption
0.07 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
ColorOpaque yellowish white-As supplied
Viscosity120,000mPa sSmall sample adapter, 25 deg C
Shelf life6monthsStored at 5 deg C
Shelf life3monthsStored at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured-material values do not share one complete cure profile.

PropertyValueUnitMethod / condition
Shore hardness80Durometer DCured material
Coefficient of linear expansion below Tg20 x 10^-6in/in/deg CCured material
Coefficient of linear expansion above Tg75 x 10^-6in/in/deg CCured material
Glass transition temperature52deg CDMTA loss of modulus
Glass transition temperature148deg CDMTA tan delta maximum
Linear cure shrinkage1.1%Cured material
Water absorption0.07%24-hour immersion
Lap shear strength1,200psiGlass to glass at 25 deg C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers