LOCTITE 404

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 404

Main features

  • Optically Clear Bondline
  • Fast Adhesive Cure
  • Low-Viscosity Adhesive Application

Product Description

LOCTITE® 404 is a one-component, low-viscosity ethyl cyanoacrylate adhesive engineered for very rapid bonding of plastics and elastomeric materials. The transparent adhesive cures quickly upon exposure to atmospheric moisture and develops handling strength within seconds on many substrates. Its fast fixture speed, excellent adhesion to plastics and rubber, and easy one-part application make it ideal for high-speed industrial assembly and maintenance operations. LOCTITE 404 is also qualified to Commercial Item Description A-A-3097, supporting its use in applications requiring recognized performance standards.

  • One-component ethyl cyanoacrylate adhesive requiring no mixing.
  • Very fast curing through ambient humidity exposure.
  • Low viscosity for rapid wetting and penetration of bonding surfaces.
  • Excellent adhesion to plastics and elastomeric materials.
  • High production efficiency due to short fixture times.
  • Transparent bond line appearance.
  • Qualified to Commercial Item Description A‑A‑3097.

Recommended Applications

  • Bonding plastics and rubber components.
  • High-speed assembly operations.
  • General industrial bonding and repair.
  • Plastic-to-plastic and plastic-to-elastomer assemblies.
  • Applications requiring very fast fixture speed.
Product Family

LOCTITE 404

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent, colorless to straw colored liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.09
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
70 - 110 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Cyanoacrylate — Ethyl cyanoacrylate adhesive
Chemical Type Ethyl Cyanoacrylate — Instant adhesive
Appearance Transparent, Colorless to Straw Colored Liquid — Uncured
Components One Part — No mixing required
Specific Gravity 1.09 — 25°C
Viscosity 70 - 110 mPa·s (cP) Brookfield LVF, Spindle 1, 30 rpm, 25°C
Key Substrates Plastics and Rubbers — Primary bonding materials
Cure Type Humidity Cure — Atmospheric moisture activated
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Glass Transition Temperature (Tg) 120 °C ASTM E228
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/m·K ISO 8302
Volume Resistivity 10 × 10¹⁵ Ω·cm IEC 60093
Dielectric Breakdown Strength 25 kV/mm IEC 60243-1
Lap Shear Strength (Steel, Grit Blasted) 18 - 26 N/mm² ISO 4587, 24 h @ 22°C
Lap Shear Strength (Aluminum) 11 - 19 N/mm² ISO 4587, Etched Aluminum
Lap Shear Strength (ABS) >6 N/mm² ISO 4587, 24 h @ 22°C
Lap Shear Strength (Neoprene) >10 N/mm² ISO 4587, 24 h @ 22°C
Tensile Strength (Steel) ≥5.2 N/mm² ISO 6922, 2 min @ 22°C