LOCTITE 3092

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 3092

Main features

  • 5 mm Gap Filling
  • Non-Sag Vertical Bonding
  • Fast Instant Fixturing

Product Description

LOCTITE 3092 is a two-part, gap-filling cyanoacrylate instant adhesive gel supplied in a 10 g/1 g twin syringe for fast bonding of common substrates. The non-sag gel stays in place on vertical surfaces and fills bond gaps up to 5 mm when dispensed through the supplied mixing nozzle. It bonds plastics, metals, rubbers, wood, paper, leather, and fabric, including porous materials that can be difficult to join with conventional liquid instant adhesives. A bonded-material temperature range of -40 deg C to 80 deg C defines the stated service boundary.

Key features

  • Gap filling to 5 mm: The mixed gel fills varying or undefined bond gaps up to 5 mm.
  • Non-sag placement: Gel consistency limits flow on vertical bonding surfaces.
  • Fast instant fixturing: The two-part system is positioned for rapid assembly of common substrates.

Applications / Suitable for

  • Bonding plastics, metals, and rubbers
  • Bonding wood, paper, leather, and fabric
  • Vertical or gap-varying assemblies up to 5 mm

Technical Specifications

General Properties
Color
The color
Clear
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
10:1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
Gel mPa.s
Thermal Properties
Temperature Resistance
Temperature resistance is the maximum temperature that the material or product can withstand for a period of time. The temperatures listed should be considered as guidelines for an operating temperature of about 30 minutes. Typically, the material can withstand much longer times at temperatures about 20°C lower and can withstand much higher temperatures for short, intermittent times.
-20 to 80 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the supplied two-part adhesive and mixed application state.

PropertyValueUnitMethod / condition
Supplied configuration10 g / 1 gtwin syringeTwo-part package
Physical formGel-Mixed adhesive
Application methodManual-Use supplied mixing nozzle
Maximum gap fill5mmMixed adhesive
Flow behaviorNon-sag-Suitable for vertical surfaces