LOCTITE 294

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 294

Main features

  • Wicking-Grade Thread Application
  • Low-Viscosity Threadlocking Application
  • High-Strength Thread Retention

Product Description

LOCTITE® 294™ is a medium-to-high-strength anaerobic threadlocking adhesive designed for the locking and sealing of pre-assembled threaded fasteners. Its low-viscosity formulation enables capillary action, allowing the adhesive to wick into engaged threads without requiring disassembly before application. The product cures when confined between closely fitting metal surfaces in the absence of air, preventing loosening and leakage caused by vibration, shock and dynamic loading. LOCTITE 294 also performs effectively on oil-coated fasteners, making it particularly suitable for maintenance, repair and production environments where disassembly is impractical.

Key Features & Benefits

  • Wicking-grade threadlocker for post-assembly application.
  • Low-viscosity formulation penetrates threads through capillary action.
  • Medium to high locking strength for threaded fasteners.
  • Prevents loosening caused by vibration, shock and dynamic loads.
  • Seals threaded assemblies against leakage.
  • Provides effective performance on oil-coated fasteners.
  • Fluorescent under UV light for inspection and quality control.

Recommended Applications

  • Post-assembly threadlocking of preassembled fasteners.
  • Maintenance and repair operations.
  • Locking of set screws and adjustment screws.
  • Sealing of threaded assemblies against leakage.
  • Equipment exposed to vibration and shock loading.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Dark green liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.13
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
20 - 45 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component adhesive
Color Dark Green — Liquid
Fluorescence Positive Under UV Light — Inspection aid
Strength Classification Medium to High — Threadlocking adhesive
Specific Gravity 1.13 — 25°C
Brookfield Viscosity 20 - 45 mPa·s LVF, spindle 2, 50 rpm, 25°C
Viscosity Classification Low — Wicking grade
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 33 N·m ISO 10964, M10 zinc phosphate steel nuts and bolts, 24 h @ 22°C
Prevail Torque 27 N·m ISO 10964, M10 zinc phosphate steel nuts and bolts, 24 h @ 22°C
Breakloose Torque 38 N·m ISO 10964, pre-torqued to 5 N·m
Maximum Prevail Torque 35 N·m ISO 10964, pre-torqued to 5 N·m
Thermal Conductivity 0.173 W/(m·K) ISO 8302
Heat Resistance Up to 260 °C After heat-aging exposure
Chemical Resistance Excellent — Resists gasoline, brake fluid, ethanol, motor oil and water/glycol mixtures
Oil-Tolerant Performance Yes — Maintains threadlocking performance on oil-coated fasteners