LOCTITE 277

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 277

Main features

  • M25 Bolt/Stud Threadlocking
  • High-Strength Thread Retention
  • Medium-Viscosity Threadlocking Application

Product Description

LOCTITE® 277 is a high-strength anaerobic threadlocking adhesive designed for the permanent locking and sealing of threaded fasteners. The one-component acrylic formulation cures when confined between closely fitting metal surfaces in the absence of air, preventing loosening and leakage caused by shock, vibration and dynamic loading. LOCTITE 277 is particularly suited for large bolts and studs (M25 and larger) where maximum holding power is required. The cured adhesive delivers excellent resistance to oils, fuels, chemicals and environmental exposure while maintaining reliable performance across a wide temperature range. Its fluorescent properties under UV light also support inspection and quality-control processes. High-strength threadlocker for permanent locking and sealing applications.

  • Prevents loosening caused by vibration, shock and dynamic loads.
  • Specifically designed for large bolts and studs (M25 and larger).
  • One-component anaerobic formulation requiring no mixing.
  • Fluorescent under UV light for inspection purposes
  • Excellent resistance to motor oil, fuel, brake fluid, water/glycol mixtures and chemicals.
  • Suitable for demanding industrial, maintenance and heavy-equipment applications.

Recommended Applications

  • Permanent locking of large threaded fasteners.
  • Heavy-duty industrial equipment and machinery.
  • Large bolts, studs and structural assemblies.
  • Equipment exposed to vibration and dynamic loading.
  • Applications requiring high resistance to chemicals and fluids.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Red liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.12
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
6,000 - 8,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component adhesive
Color Red — Liquid
Fluorescence Positive Under UV Light — Inspection aid
Specific Gravity 1.12 — 25°C
Brookfield Viscosity 6,000 - 8,000 mPa·s RVT, spindle 4, 20 rpm, 25°C
Strength Classification High — Threadlocking adhesive
Flash Point 165 °C Cleveland Open Cup
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 32 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Prevail Torque 32 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Breakloose Torque 38 N·m ISO 10964, pre-torqued to 5 N·m
Maximum Prevail Torque 40 N·m ISO 10964, pre-torqued to 5 N·m
Compressive Shear Strength ≥9 N/mm² ISO 10123, steel pins and collars
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Cold Temperature Capability -75 °C Tested minimum temperature
Chemical Resistance Excellent — Resists motor oil, gasoline, brake fluid, ethanol and industrial chemicals

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers