LOCTITE 2760

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 2760

Main features

  • Fast Anaerobic Cure
  • High-Strength Heavy-Duty Locking
  • Reduced Liquid Migration

Product Description

LOCTITE 2760 is a red, one-component anaerobic threadlocker for high-strength retention of heavy-duty metal fasteners. The medium-thixotropic liquid cures without air between close-fitting metal surfaces and is formulated for fast cure, reducing the need for activator on many assemblies. Its controlled flow helps limit migration after application. LOCTITE 2760 is suited to threaded joints exposed to high shock and stress, including bolts used in transmissions, construction equipment, and railroad assemblies. Torque performance is specific to defined steel fastener sizes, pretightening conditions, temperatures, and cure times.

Key features

  • Fast anaerobic cure: The formulation develops strength quickly on close-fitting metal threads.
  • High-strength locking: Cured joints are intended for heavy-duty shock- and stress-loaded fasteners.
  • Reduced liquid migration: Medium thixotropy helps keep the applied product at the thread area.

Applications / Suitable for

  • Transmission fasteners
  • Construction equipment bolts
  • Railroad assemblies and other heavy-duty threaded joints

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Liquid
Chemistry Type
Dimethacrylate ester
Color
The color
Red
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
1K
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.15
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,250 to 4,250 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
AppearanceRed homogeneous liquid-Uncured
ComponentsOne-No mixing required
Cure mechanismAnaerobic-Secondary cure with activator when required
Specific gravity1.15-Typical at 25 deg C
Viscosity1,250 to 4,250mPa sBrookfield RVT, spindle 3, 20 rpm, 25 deg C
FluorescencePositive-Visible under UV light
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakaway torque>=8N mISO 10964; 3/8 x 16 grade 2 nuts and grade 5 bolts; cured 4 h at 22 deg C
Prevail torque>=10.1N mISO 10964; 3/8 x 16 grade 2 nuts and grade 5 bolts; cured 4 h at 22 deg C
Breakaway torque>=11.3N mISO 10964; 3/8 x 16 grade 2 nuts and grade 5 bolts; cured 24 h at 22 deg C
Prevail torque>=14.1N mISO 10964; 3/8 x 16 grade 2 nuts and grade 5 bolts; cured 24 h at 22 deg C
Breakloose torque36.7N mISO 10964; pretorqued 5 N m; 3/8 x 16 steel; cured 24 h at 22 deg C
Maximum prevail torque36.1N mISO 10964; pretorqued 5 N m; 3/8 x 16 steel; cured 24 h at 22 deg C