LOCTITE® 272™ is a high-strength anaerobic threadlocking adhesive formulated for the permanent locking and sealing of threaded metal fasteners. The one-component acrylic adhesive cures when confined between closely fitting metal surfaces in the absence of air, preventing loosening and leakage caused by vibration, shock and dynamic loading. Designed for demanding industrial environments, LOCTITE 272 is particularly suitable for locking and sealing large bolts and studs M25 and larger. Its high-temperature resistance, chemical durability and strong retention performance make it ideal for heavy equipment, industrial machinery and high-heat service applications.

Key Features & Benefits

  • High-strength threadlocker for permanent locking and sealing.
  • Prevents loosening caused by shock, vibration and dynamic loading.
  • Designed for large bolts and studs including M25 and larger fasteners.
  • Excellent high-temperature performance and retention strength.
  • One-component anaerobic formulation requiring no mixing.
  • Provides resistance to oils, gasoline, water and industrial chemicals.
  • Suitable for heavy-duty industrial and maintenance applications.

Recommended Applications

  • Large bolts and stud assemblies.
  • Heavy industrial machinery and process equipment.
  • Power generation and high-temperature service environments.
  • Permanent threadlocking and thread sealing applications.
  • Equipment exposed to vibration, shock and elevated operating temperatures.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Red-orange liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.11
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
4,000 - 15,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component adhesive
Appearance Red-Orange Liquid — Uncured
Strength Classification High — Threadlocking adhesive
Specific Gravity 1.11 — 25°C
Brookfield Viscosity 4,000 - 15,000 mPa·s RVT, spindle 4, 20 rpm, 25°C
Density 1.11 g/cm³ 20°C
Flash Point >100 °C Closed cup
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 23 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Prevail Torque 25 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Compressive Shear Strength ≥14.5 N/mm² ISO 10123, steel pins and collars, 24 h @ 22°C
Compressive Shear Strength ≥20 N/mm² After 72 h at 200°C, tested at 200°C
Coefficient of Thermal Expansion 80 × 10⁻⁶ K⁻¹ ISO 11359-2
Thermal Conductivity 0.1 W/(m·K) ISO 8302
Specific Heat 0.3 kJ/(kg·K) Typical cured value
Heat Resistance Up to 200 °C Hot strength and aging performance