LOCTITE 271

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 271

Main features

  • High-Strength Thread Retention
  • Low-Viscosity Threadlocking Application
  • Large Threaded-Fastener Locking

Product Description

LOCTITE® 271™ is a high-strength anaerobic threadlocking adhesive formulated for the permanent locking and sealing of threaded metal fasteners. The one-component acrylic adhesive cures when confined between closely fitting metal surfaces and isolated from air, preventing loosening and leakage caused by vibration, shock and dynamic loading. LOCTITE 271 is particularly suitable for large bolts and studs up to M25 and provides excellent retention strength for applications where disassembly is not intended. The low-viscosity formulation delivers dependable performance across a wide range of industrial environments while offering resistance to oils, fuels, solvents and elevated temperatures.

Key Features & Benefits

  • High-strength threadlocker for permanent fastener locking and sealing.
  • Prevents loosening caused by vibration, shock and impact loads.
  • Suitable for large threaded fasteners and studs up to M25.
  • Low-viscosity formulation promotes efficient thread penetration.
  • One-component anaerobic adhesive requiring no mixing.
  • Resistant to oils, fuels, solvents and industrial fluids.
  • Fluorescent under UV light for inspection and quality verification.

Recommended Applications

  • Permanent locking of threaded fasteners.
  • Large bolts, studs and heavy-duty threaded assemblies.
  • Industrial machinery and equipment assembly.
  • Automotive and transportation maintenance applications.
  • Threaded joints exposed to vibration and dynamic loads.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Red
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
400 - 600 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component
Color Red — Liquid
Strength Classification High — Threadlocking adhesive
Fluorescence Positive — Visible under UV light
Specific Gravity 1.10 — 25°C
Viscosity 400 - 600 mPa·s Brookfield RVT, spindle 1, 10 rpm, 25°C
Flash Point >100 °C See SDS
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 17 - 40 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Prevail Torque 23 - 40 N·m ISO 10964, M10 steel nuts and bolts, 24 h @ 22°C
Breakaway Torque (90 min) 8.5 - 25.4 N·m ISO 10964, steel nuts and bolts, 90 min @ 22°C
Prevail Torque (90 min) 16.9 - 34 N·m ISO 10964, steel nuts and bolts, 90 min @ 22°C
Heat Resistance Up to 150 °C Hot strength testing
Chemical Resistance Excellent — Resists motor oil, fuels, brake fluid, ethanol and solvents
Strength Retention in Motor Oil 75 % After 1,000 h exposure at 125°C
Recommended Disassembly Temperature 250 °C Apply localized heat before removal