LOCTITE 268

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 268 LOCTITE 268 LOCTITE 268

Main features

  • High-Strength Thread Retention
  • Self-Feeding Stick Control
  • Active and Passive Metal Cure

Product Description

LOCTITE 268 is a red, wax-consistency anaerobic threadlocker supplied in a self-feeding stick for high-strength locking of metal fasteners. The semi-solid format supports direct contact with threaded parts and controlled coverage where a liquid grade may be too fluid or difficult to apply. It cures without air between close-fitting metal surfaces and develops strength on active metals such as brass and copper as well as passive surfaces including stainless steel and plated fasteners. UV fluorescence supports application inspection. Torque values apply to degreased steel, black-oxide steel, and stainless-steel assemblies under defined cure schedules.

Key features

  • High-strength retention: The cured threadlocker is intended for fasteners requiring durable locking strength.
  • Self-feeding stick control: The wax-like semi-solid format supports direct and even application to threads.
  • Broad metal cure: The anaerobic system develops strength on active and passive metal substrates.

Applications / Suitable for

  • High-strength locking of active and passive metal fasteners
  • Stainless steel and plated threaded assemblies
  • Applications where semi-solid stick placement is preferred

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Stick
Chemistry Type
Dimethacrylate ester
Color
The color
Red
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
1K
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.03
Chemical Properties
Melting Point
>65 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
Appearance and formRed wax-consistency stick-Uncured
ComponentsOne-No mixing required
FluorescencePositive-Visible under UV light
Specific gravity1.03-Typical at 25 deg C
Unworked penetration90 to 1500.1 mmISO 2137
Melting point>65deg CTypical
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakloose torque>=8N mISO 10964; pretorqued 5 N m; degreased 3/8 x 16 steel; cured 1 h at 25 deg C
Breakloose torque>=8N mISO 10964; pretorqued 5 N m; degreased stainless 3/8 x 16; cured 4 h at 25 deg C
Breakaway torque10N mISO 10964; degreased 3/8 x 16 steel; cured 24 h at 22 deg C
Breakaway torque16N mISO 10964; degreased stainless 3/8 x 16; cured 24 h at 22 deg C
Breakloose torque>=17N mISO 10964; pretorqued 5 N m; degreased 3/8 x 16 steel; cured 24 h at 22 deg C
Breakloose torque40N mISO 10964; pretorqued 5 N m; degreased M10 black-oxide steel; cured 24 h at 22 deg C
Breakloose torque23N mISO 10964; pretorqued 5 N m; degreased stainless 3/8 x 16; cured 24 h at 22 deg C

Leading Brands Trust in Our Products and Services