LOCTITE 262

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 262

Main features

  • One-Component Threadlocking System
  • High-Strength Thread Retention
  • Thixotropic Application Control

Product Description

LOCTITE® 262™ is a medium to high-strength anaerobic threadlocking adhesive designed for the permanent locking and sealing of threaded metal fasteners. The one-component acrylic formulation cures in the absence of air between closely fitting metal surfaces to prevent loosening and leakage caused by shock and vibration. LOCTITE 262 is particularly suitable for locking and sealing large bolts and studs up to M25 size and features a thixotropic consistency that minimizes migration after application. The cured adhesive delivers reliable resistance to heat, oils, fuels, brake fluids and other industrial fluids while providing dependable fastener retention in demanding environments.

Key Features & Benefits

  • Medium to high-strength threadlocker for permanent fastener locking.
  • Prevents loosening and leakage caused by vibration and shock.
  • Suitable for large bolts and threaded studs up to M25.
  • Thixotropic formulation minimizes migration after application.
  • One-component anaerobic adhesive requiring no mixing.
  • Provides excellent resistance to oils, fuels, brake fluid and industrial chemicals.
  • Fluorescent under UV light for inspection and quality control.

Recommended Applications

  • Permanent locking of threaded fasteners.
  • Sealing threaded assemblies against leakage.
  • Large bolts, studs and heavy-duty threaded connections.
  • Industrial machinery and equipment assembly.
  • Automotive, transportation and maintenance applications.

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,200 - 1,400 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate Ester — One-component
Color Red — Liquid
Fluorescence Positive — Visible under UV light
Viscosity 1,200 - 1,400 mPa·s Brookfield RVT, 25°C
Specific Gravity 1.10 — 25°C
Density 1.05 g/ml 20°C
Flash Point >100 °C Closed cup
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 22 N·m ISO 10964, M10 steel nuts & bolts, 24 h @ 22°C
Prevail Torque 38 N·m ISO 10964, M10 steel nuts & bolts
Breakloose Torque 32 N·m ISO 10964, pre-torqued to 5 N·m
Maximum Prevail Torque 40 N·m ISO 10964, pre-torqued to 5 N·m
Compressive Shear Strength ≥10 N/mm² ISO 10123, steel pins & collars, 24 h @ 22°C
Compressive Shear Strength ≥3 N/mm² ISO 10123, steel pins & collars, 1 h @ 22°C
Strength Classification Medium to High — Threadlocking performance
Heat Resistance Up to 150 °C Environmental aging data