LOCTITE 248

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 248 LOCTITE 248 LOCTITE 248

Main features

  • Clean Stick Application
  • Medium-Strength Metal Threadlocking
  • Active and Passive Metal Cure

Product Description

LOCTITE 248 is a blue, wax-consistency anaerobic threadlocker supplied in a self-feeding stick for medium-strength locking of metal fasteners. The semi-solid format allows direct application to threads and is useful where a liquid product may be too fluid or difficult to place. It cures when confined between close-fitting metal surfaces without air and works on active metals as well as passive surfaces such as stainless steel and plated fasteners. UV fluorescence supports application inspection. Torque values apply to degreased steel, black-oxide steel, and stainless-steel fastener configurations under defined cure conditions.

Key features

  • Clean stick application: The self-feeding semi-solid format supports direct, controlled placement on threads.
  • Active and passive metals: The anaerobic formulation cures on common active metals and passive metal surfaces.
  • Medium-strength retention: Cured assemblies provide threadlocking while remaining serviceable with appropriate tools.

Applications / Suitable for

  • Medium-strength locking of metal fasteners
  • Stainless steel and plated threaded assemblies
  • Applications where stick placement is preferred over liquid

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Stick
Chemistry Type
Dimethacrylate ester
Color
The color
Blue
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
1K
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.03
Chemical Properties
Melting Point
>65 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the product before cure or assembly.

PropertyValueUnitMethod / condition
Appearance and formBlue wax-consistency stick-Uncured
ComponentsOne-No mixing required
FluorescencePositive-Visible under UV light
Specific gravity1.03-Typical
Unworked penetration90 to 1400.1 mmISO 2137
Melting point>65deg CTypical
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed conditions.

PropertyValueUnitMethod / condition
Breakloose torque>=7N mISO 10964; pretorqued 5 N m; degreased 3/8 x 16 steel; cured 1 h at 25 deg C
Breakloose torque>=6N mISO 10964; pretorqued 5 N m; stainless 3/8 x 16; cured 4 h at 25 deg C
Breakaway torque13N mISO 10964; degreased 3/8 x 16 steel; cured 24 h at 25 deg C
Breakaway torque23N mISO 10964; M10 black-oxide steel; cured 24 h at 25 deg C
Breakaway torque12N mISO 10964; stainless 3/8 x 16; cured 24 h at 25 deg C
Breakloose torque25N mISO 10964; pretorqued 5 N m; M10 black-oxide steel; cured 24 h at 25 deg C