Product Description

LOCTITE® 2047™ is a one-component anaerobic threadlocker formulated for high-strength locking of threaded fasteners while providing enhanced lubricity. Designed for assemblies requiring reliable resistance to loosening and leakage caused by shock and vibration, the product cures when confined between closely fitting metal surfaces in the absence of air. Its specialized lubricant additives provide lubricity comparable to conventional metal-free anti-seize products while maintaining threadlocking performance. LOCTITE 2047 features a deliberately slow cure profile that allows multiple fasteners to be torqued in large assemblies before curing begins, making it particularly suitable for large, highly torqued bolt applications where assembly-generated heat could otherwise cause premature curing.

Key Features & Benefits

  • High-strength anaerobic threadlocker for metal threaded fasteners.
  • Contains lubricant additives that provide lubricity comparable to metal-free anti-seize compounds.
  • Prevents loosening and leakage caused by shock and vibration.
  • One-component formulation requiring no mixing before use.
  • Slow cure profile allows sequential torquing of multiple bolts before cure initiation.
  • Suitable for large, highly torqued fasteners where assembly heat may otherwise induce premature cure.

Recommended Applications

  • High-strength threadlocking of nuts and bolts.
  • Threaded assemblies exposed to vibration and shock loading.
  • Large-diameter and highly torqued bolted assemblies.
  • Thread sealing applications requiring leak prevention.
  • Industrial maintenance, assembly and heavy equipment fastening.

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,000 - 12,000 mPa.s

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Technology Acrylic — Anaerobic threadlocker
Chemical Type Dimethacrylate ester — Product composition
Appearance Black liquid — Uncured
Components One-component — No mixing required
Viscosity 2,000 - 12,000 mPa·s (cP) Brookfield RVT, 25°C
Density 1.115 g/cm³ 27°C
Flash Point >93 °C Pensky-Martens closed cup
Boiling Point >149 °C Typical value
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Breakaway Torque 43 N·m ISO 10964, steel nuts & bolts, 72 h @ 22°C
Breakloose Torque 35 N·m ISO 10964, steel nuts & bolts, pre-torqued to 5 N·m
Prevail Torque 9 N·m ISO 10964, 72 h @ 22°C
Prevail Torque (Pre-torqued) 7 N·m ISO 10964, pre-torqued to 5 N·m
Compressive Shear Strength 24.5 N/mm² ISO 10123, steel pins and collars
Lubricity K-Factor (3/8 x 16) 0.15 — Zinc plated steel nuts and bolts
Lubricity K-Factor (5/8 x 11) 0.14 — Zinc plated steel nuts and bolts
Lubricity K-Factor (7/8 x 9) 0.13 — Zinc plated steel nuts and bolts