Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE 190017

Main features

  • Anaerobic Adhesive Technology
  • Above 100 deg C Flash Point
  • Clear Liquid Formulation

Product Description

LOCTITE 190017 1L EN is a clear, liquid anaerobic adhesive formulated for bonding and locking applications where curing occurs in the absence of air between closely fitting metal surfaces. The product exhibits a mild acrylic odor, a density of approximately 1.23 g/cm³, and a flash point greater than 100°C. Its liquid consistency supports dispensing and application in threaded assembly and retaining operations where anaerobic adhesive technology is commonly used. The material is supplied as a clear liquid and remains stable under recommended storage conditions. It is classified as a skin sensitizer and should be handled using appropriate industrial hygiene and personal-protection practices.

Key features

  • Anaerobic adhesive technology: Designed to cure in the absence of air for locking and bonding applications.
  • High flash point: Flash point greater than 100°C supports safer handling compared with lower-flash-point materials.
  • Clear liquid formulation: Liquid delivery form supports controlled dispensing during assembly operations.

Technical Specifications

General Properties
Density (g)
1.17 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
5,000 - 9,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Physical properties of LOCTITE 190017 1L EN in its supplied liquid state.

Property Value Unit Method / condition
Technology Anaerobic adhesive — Product classification
Appearance Clear liquid — Delivery form
Density 1.2301 g/cm³ 20°C
Flash point >100 °C Tagliabue closed cup
Kinematic viscosity >20.5 mm²/s 40°C
Initial boiling point >150 °C Physical property