LOCTITE 122S

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LOCTITE 122S

Main features

  • Thixotropic Application Control
  • Non-Staining Mold Release Formulation
  • Non-Flammable Mold Release Formulation

Product Description

LOCTITE 122S RD E&C is a silicone-based mold release grease with a pink, thixotropic paste consistency designed for molding applications where controlled release is required. The material is applied by wiping or brushing onto mold surfaces and air dries to a dry-to-touch film in approximately 5 to 10 minutes at 25°C. Its non-staining, non-flammable, and non-corrosive characteristics support use in manufacturing environments where clean mold release performance and elevated-temperature physical stability are important. The product is intended for selective application to mold surfaces requiring release properties and should not be applied to surfaces that will later be bonded.

Key features

  • Thixotropic silicone grease: Paste consistency enables controlled, selective application to mold surfaces.
  • Fast air-dry behavior: Dries to the touch in approximately 5 to 10 minutes at 25°C.
  • Non-staining and non-corrosive: Supports mold release operations while helping maintain surface condition.

Applications / Suitable for

  • Molding applications requiring a paste-consistency mold release.
  • Selective mold-surface treatment using a brush or cloth.
  • Processes requiring air-dried mold release films.

Technical Specifications

General Properties
Density (g)
0.99 g/cm3

Additional Information

Technical properties

As-supplied / before-processing properties

Representative as-supplied properties for LOCTITE 122S RD E&C prior to application and drying.

Property Value Unit Method / condition
Technology Silicone — As supplied
Appearance Pink grease — Visual description
Density 0.99 g/cm³ ASTM D792
Shelf life 548 days 25°C
Recommended drying time 5–10 minutes 25°C, dry to touch