LOCTITE 087

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LOCTITE 087 LOCTITE 087

Main features

  • High-Strength Coarse-Thread Retention
  • 11.3 to 28.3 N m Prevail Torque
  • One-Part Heat-Assisted Disassembly

Product Description

LOCTITE GRD AV High-Strength Threadlocker is a one-part red anaerobic liquid for locking and sealing large, coarse-threaded nuts, bolts, and studs. Its 100 to 250 mPa s viscosity supports controlled application before assembly, and the high-strength cured bond is intended for fasteners requiring durable retention. After 24 hours at 22 deg C, it develops 7 N m breakaway torque and 11.3 to 28.3 N m prevail torque on 3/8 x 24 grade 2 steel fasteners under ISO 10964 testing. The product requires no mixing; disassembly is performed with localized heat when removal is necessary. Applications include large coarse-threaded metal assemblies where high locking strength is required.

Key features

  • High-Strength Coarse-Thread Locking: The red anaerobic liquid is intended for large coarse-threaded fasteners requiring high locking strength.
  • 11.3 to 28.3 N m Prevail Torque: Typical prevail torque is measured after 24 hours at 22 deg C on grade 2 steel fasteners.
  • Heat-Assisted Disassembly: Localized heat enables removal when the high-strength threaded assembly must be disassembled.

Applications / Suitable for

  • Large coarse-threaded nuts, bolts, and studs
  • High-strength metal fastener retention
  • Threaded assemblies requiring locking and sealing

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Liquid
Chemistry Type
Dimethacrylate ester
Color
The color
Red
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
1K
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.07
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
100 to 250 mPa.s
Thermal Properties
Specific Heat Capacity
Specific heat capacity is the amount of heat energy required to raise the temperature of a substance per unit of mass. The specific heat capacity of a material is a physical property. It is also an example of an extensive property since its value is proportional to the size of the system being examined.
300 J/(g⋅°C)
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.1 W/m.K
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
9.8 kV/mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured and storage properties for LOCTITE GRD AV.

Property Value Unit Method / condition
Appearance Red liquid Uncured material; LMS
Components One component No mixing required
Viscosity 100 to 250 mPa s Cannon-Fenske; ISO 3104; uncured material
Specific gravity 1.07 At 25 deg C; uncured material
Cure mechanism Anaerobic Threadlocking application
Optimal storage 8 to 21 deg C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Typical cured-material and threaded-fastener results for LOCTITE GRD AV.

Property Value Unit Method / condition
Breakaway torque 7 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Prevail torque 11.3 to 28.3 N m After 24 hours at 22 deg C; ISO 10964; 3/8 x 24 grade 2 steel nuts and bolts
Dielectric breakdown strength 9.8 kV/mm IEC 60243-1; cured material
Thermal conductivity 0.1 W/(m K) ISO 8302; cured material
Coefficient of thermal expansion 100 x 10^-6 K^-1 ISO 11359-2; cured material
Specific heat 0.3 kJ/(kg K) Cured material