MVCF-8S50K | LINQSTAT 8mil - 50,000 Ω/sq Conductive Film

Harmonization Code : 3920.10.89.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials; Of polymers of ethylene; Of a thickness exceeding 0,125 mm; Other; Other; Other

LINQSTAT MVCF - Short Roll MVCF-8S50K | LINQSTAT 8mil - 50,000 Ω/sq Conductive Film

Main features

  • 8 mil - 203um - 0.2mm
  • ±50,000 ohms/sq Surface resistivity
  • ±TBD ohms/cm Volume resistivity

Product Description

LINQSTAT MVCF-8S50K is a black, carbon-filled, electrically conductive polyethylene plastic film designed to provide both physical and static protection. Having a surface resistivity below 5 x 104 Ω/sq it offers medium-level static protection which means it effectively avoids accumulation of electric charge on itself and the products which it protects. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. Please keep in mind that 50,000 ohms/sq is not an absolute value by any means. These are not meant to be highly controlled sheets as reflected on their price range. The guaranteed property is that it is going to be around or below 50,000ohms/sq with a 10-20k tolerance downwards.

MVCF-8S50K is useful in applications where the key is to balance cost versus performance. As a medium-level conductive plastic, the carbon-loading is such that it is low-enough to be cost effective, while being high enough to meet the electrical requirements of military specification MIL-PRF-81705D Type II and MIL-P-82646A. Please note that  Linqstat  MVCF-8S50K is surface conductive and the volume conductivity still needs to be determined.

MVCF-8S50K plastic film and its conductivity are unaffected by humidity and age. The film is heat sealable, flexible and offers exceptional abrasion resistance. To add to that, it exhibits good thermal stability and has outstanding chemical resistance. It is available in 8 mil (0.2mm). Other thicknesses can be available upon request. Additionally, the film has been proven to be highly UV resistant, absorbing UV radiation at 365 nm up to 100%.

Production batches from 2023 will have a tolerance of ±40,000ohms

Product Family

LINQ MVCF-8S50K

1. Select Width
2. Select Length

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Carbon-Loaded PE
Color
The color
Black
Density (g)
1 g/cm3
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.2 mm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.1
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.053 W/m.K
Electrical Properties
Surface Resistivity
50000 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
TBD Ohms⋅cm
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
360 %

Additional Information

In sheet form, the conductive polyethylene is used as a weak pressure sensor making it useful for applications that have large surface areas and expect large pressure applications. For more sensitive pressure sensor applications, KRAYDEN recommends LINQSTAT XVCF-Series, which is a more conductive series of polyethylene plastics.

As an antistatic packaging plastic, it is also used as an antistatic interleaver for Smartcard (micromodule) applications to separate subsequent layers of smartcard chips in micromodule production. It’s antistatic properties make the Linqstat MVCF series films also well suited for EMI and RF shielding applications.

Product Applications

  • EMI/RF Shielding
  • Large Pressure Sensors
  • Faraday Cages

Product Features and Benefits

  • Black Opaque - Printable
  • Provides Anti-Static protection to electronics components
  • Groundable
  • Humidity independent conductivity
  • Meets military specification MIL-P-82646A

Chemical Susceptibility

  • Methanol: Resistant
  • Ethanol: Resistant
  • Isopropanol: Resistant
  • Weak Acids: Resistant
  • Ketones (Acetone): Slow Attack
  • Weak Alkalines: Slow Attack
  • Hydrocarbons: Non-Resistant