LENIUM ES

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LENIUM ES

Main features

  • Electronics Defluxing and Decontamination
  • Broad Multi-Soil Cleaning Range
  • Qualified Solvent-Replacement Scope

Product Description

LENIUM™ ES is a binary azeotrope of n-propyl bromide (nPB), isopropyl alcohol (IPA), and stabilizers designed for open-top and vacuum vapor degreasers. It is formulated for electronics defluxing, including removal of solder flux residues and ionic contamination from circuit assemblies, and also removes documented industrial soils such as adhesives, buffing compounds, drawing oils, greases, hydraulic oils, lapping compounds, resins, inks, silicone oils, and waxes. Current typical data include a 148–151°F (64–66°C) boiling range, 0.49 cP viscosity at 20°C, 110.9 mm Hg vapor pressure at 20°C, and a Kauri-Butanol value of 125.

Key features

  • Electronics defluxing: Removes solder flux residues and ionic contamination from circuit assemblies in vapor-degreasing processes.
  • Broad documented soil removal: Removes adhesives, buffing compounds, drawing oils, greases, hydraulic oils, lapping compounds, resins, inks, silicone oils, and waxes.
  • Open-top and vacuum equipment fit: Designed for use in both open-top and vacuum vapor degreasers.
  • Defined process-control data: The current TDS provides controller references including LTC 164°F (73°C), HTC 169°F (76°C), SVC/VU 144°F (62°C), and primary refrigeration at 35–40°F (2–5°C).
  • Legacy-solvent replacement scope: Supplier-positioned as a drop-in replacement for TCE, HCFC-141b, HCFC-225, PCE, and methylene chloride.
  • Qualification support: Current Vantage product information lists Goodrich Landing LGPS 1400, Lockheed Martin EMAP G41.149, and Safran In-1500 approval references.

Applications / Suitable for

  • Electronics and PCBA defluxing
  • Precision cleaning in vapor-degreasing equipment
  • Military and defense cleaning processes within the applicable approval and process scope
Product Family

LENIUM ES

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.25
Vapor Pressure
110.9 mmHg
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
64-66 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
None °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.49 mPa.s

Additional Information

Surface Treatments | Vapor-Degreasing & Defluxing Solution

LENIUM™ ES

LENIUM ES is a stabilized nPB/IPA vapor-degreasing solution for electronics defluxing and precision cleaning. It is designed for open-top and vacuum vapor degreasers, removes solder flux residues and ionic contamination from circuit assemblies, and also addresses a broad range of documented industrial soils.

nPB + IPA azeotrope Electronics defluxing Open-top & vacuum systems 148–151°F boiling range 0.49 cP at 20°C KB value 125

Vantage Drum Packaging

As-Supplied Properties

Boiling range
148–151°F (64–66°C)
Decision-relevant physical data for vapor-degreasing process evaluation; it is not itself a universal equipment setpoint.
Viscosity
0.49 cP at 20°C
Typical liquid viscosity reported in the current technical data sheet.
Kauri-Butanol value
125
Typical solvency-index value used alongside the documented soil-removal scope.

Typical data is provided for product evaluation and is not intended as a guaranteed specification unless explicitly identified as such by the manufacturer.

Property Value Unit Method / condition
Appearance Clear liquid — As supplied
Specific gravity 1.25 — At 25°C
Flash point None — Reported in the current TDS; no additional flash-point method is stated in the table
Boiling point 148–151 (64–66) °F (°C) Typical boiling range
Viscosity 0.49 cP At 20°C
Vapor pressure 110.9 mm Hg At 20°C
Evaporation rate 0.96 TCA = 1 Relative evaporation rate
Specific heat 0.27 — At 25°C; unit is not stated in the current TDS table
Heat of vaporization 58.8 cal/g Typical value
Kauri-Butanol value 125 — Typical solvency index
Processing

Vapor-Degreasing Process

LENIUM ES is designed for open-top and vacuum vapor degreasers. The current technical data sheet directs users to add the product at full concentration to the tank reservoir or reservoirs and provides controller references for process setup. Use the current Vantage operating manual and equipment-specific instructions for the complete operating procedure.

Charge concentration: Add LENIUM ES at full concentration to the tank reservoir(s).
Controller references: Liquid Temperature Controller (LTC) 164°F (73°C); High Temperature Controller (HTC) 169°F (76°C); Safety Vapor Controller (SVC) 144°F (62°C); Vapor Up Temperature (VU) 144°F (62°C).
Primary refrigeration: 35–40°F (2–5°C).
Cleaning role: Supports electronics defluxing and precision cleaning, including removal of solder flux residues, ionic contamination, and the other documented soil types.
 
Storage and Handling

LENIUM ES has a 36-month shelf life when stored in the original, sealed container above 50°F (10°C). Current Vantage technical data lists 50 lb (23 kg) pails and 550 lb (249 kg) drums. Consult the current Safety Data Sheet and applicable workplace, transport, environmental, and equipment requirements for complete handling, exposure-control, storage, and disposal information.

Qualification and Approval References

Current Vantage product information lists the following approval references for LENIUM ES. Applicability remains controlled by the exact specification, process, revision, substrate or assembly, facility, and acceptance requirements.

Current listed approval references
  • Goodrich Landing LGPS 1400 Solvent Cleaning / Degreasing
  • Lockheed Martin EMAP G41.149
  • Safran In-1500 Products Used For Degreasing-Organic Solvents (n-Propyl Bromide)
Confirm the current revision and the exact controlled-process applicability before specification or release.
Defined legacy-solvent replacement scope
Vantage positions LENIUM ES as a drop-in replacement for trichloroethylene (TCE), HCFC-141b, HCFC-225, perchloroethylene (PCE), and methylene chloride (MeCl).
Replacement language is limited to the named solvents and does not remove the need to verify actual equipment, material compatibility, cleaning performance, residues, exposure controls, and process qualification.
Use contexts

Applications

Evaluate LENIUM ES within the documented vapor-degreasing, soil-removal, material, approval, cleanliness, and safety boundaries. Application trials should represent the actual assembly materials, contaminant set, equipment, cycle, and downstream process requirements.

Electronics and PCBA defluxing
Use in vapor-degreasing processes to remove solder flux residues and ionic contamination from circuit assemblies, with cleaning performance and material compatibility verified on the actual assembly.
Precision parts cleaning
Evaluate for removing documented industrial soils including adhesives, buffing and lapping compounds, drawing and hydraulic oils, greases, resins, inks, silicone oils, and waxes in open-top or vacuum vapor-degreasing equipment.
Military and defense cleaning
The current Vantage product page identifies Military & Defense as an application area. Use within the exact approval, specification, equipment, part-material, and cleanliness requirements that govern the intended process.

Product Resources

Electronics Cleaning Solutions Brochure
Vantage brochure covering electronics-cleaning technologies, including LENIUM ES positioning for nPB vapor degreasing and defluxing.
View resource
Aerospace and Defense Brochure
Vantage overview of surface-treatment solutions for aerospace and defense, including LENIUM vapor-degreasing products and application context.
View resource
Next steps

Technical Support

Work with Krayden to evaluate LENIUM ES against your vapor-degreasing equipment, flux or soil set, assembly materials, controller requirements, cleanliness targets, approval scope, packaging, and safety controls. Krayden can help coordinate technical review, application testing, and process implementation with Vantage.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers