LAIRD TPUTTY 506

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD TPUTTY 506

Main features

  • No-Cure Single-Part Putty
  • 3.5 W/m-K Thermal Conductivity
  • Low-Pressure Uneven-Gap Filling

Product Description

Tputty 506 Thermal Gap Filler Putty is a soft, single-part silicone material for dispensing into large and uneven electronic thermal gaps without a cure step. Its ceramic-filled formulation provides 3.5 W/(m K) thermal conductivity while transferring little pressure between mating surfaces. The putty is more viscous than grease and uses specialized rheology for controlled flow under pressure, supporting application through dispensing equipment. A minimum bondline thickness of 0.1 mm and a -45 to 200 deg C operating range support varied interface geometries. Applications include microprocessors, graphics chips, automotive electronics, and LED lighting assemblies.

Key features

  • No-Cure Single-Part Putty: The dispensable silicone material fills large and uneven gaps without curing.
  • 3.5 W/(m K) Thermal Conductivity: Ceramic-filled putty transfers heat while remaining soft and compliant.
  • Low-Pressure Uneven-Gap Filling: Specialized rheology supports controlled flow with little pressure transfer.

Applications / Suitable for

  • Microprocessors and graphics chips
  • Automotive electronics
  • LED lighting assemblies
Product Family

LAIRD TPUTTY 506

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Fully Cured Ceramic-filled dispensable silicone putty
Density (g)
1.71 g/cm3
Thermal Properties
Operating Temperature
(-)45 to 200 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.5 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied dispensing and material properties for Tputty 506.

Property Value Unit Method / condition
Construction Ceramic-filled dispensable silicone putty Single-part; no cure required
Color Turquoise Visual
Flow rate 17.2 cc/min 75 cc taper tip; 0.125 inch orifice; 90 psi
Density 1.71 g/cc Helium pycnometer
Filler abrasiveness 2 Mohs Predominant filler
Available packages 75, 180, 360, 600 cc Dispensing cartridges
Bulk package 20 kg Pail
Technical properties

After-processing / final-state properties

Typical installed-interface properties for the non-curing Tputty 506 material.

Property Value Unit Method / condition
Thermal conductivity 3.5 W/(m K) Hot Disk
Operating temperature range -45 to 200 deg C Specified operating range
Minimum bondline thickness 0.1 mm 0.004 inch
Volume resistivity 1.8 x 10^14 ohm cm Typical bulk property
Outgassing TML 0.46 % by weight ASTM E595
Coefficient of thermal expansion 227 ppm/K Volume dilatometry
Glass transition temperature less than -90 deg C ASTM E1356
Flammability V-0 UL 94