LAIRD TGON 805

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

LAIRD TGON 805

Main features

  • 0.13 mm Flexible Graphite Interface
  • 5 W/(m K) Through-Plane Conductivity
  • 0.07 deg C in^2/W Thermal Resistance

Product Description

Laird Tgon™ 805 is the 0.13 mm-thick configuration of the Tgon™ 800 Series, a flexible graphite interface pad designed for applications where electrical isolation is not required and both electrical contact and thermal transfer are desired. Its grain-oriented, plate-like graphite structure provides typical thermal conductivity of 5 W/m·K through the Z axis and 240 W/m·K in the X-Y plane. The material contains more than 98% graphite and is available without adhesive or with a thin pressure-sensitive adhesive on one side to aid assembly.

Key Features

  • 0.13 mm nominal thickness for thin electrically and thermally conductive interfaces.
  • Anisotropic thermal conductivity of 5 W/m·K through-plane and 240 W/m·K in-plane.
  • More than 98% graphite construction with low thermal resistance and optional one-side pressure-sensitive adhesive.

Applications / Suitable for

  • Power conversion equipment
  • Power supplies
  • Large telecommunications switching hardware
  • Notebook computers
  • Applications requiring electrical grounding with thermal conductivity

Technical Specifications

General Properties
Color
The color
Pewter
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Flexible Graphite
Density (g)
2.2 g/cm3
Thickness range
0.13 mm
Thermal Properties
Operating Temperature
-240 to 300 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
5 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
11 x 10^-5 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for the 0.13 mm Tgon™ 805 configuration of the Tgon™ 800 Series.

Property Value Unit Method / condition
Construction Flexible graphite — Typical specification
Color Pewter — Visual
Nominal thickness 0.005 in Equivalent to 0.13 mm
Thickness tolerance ±0.001 in Equivalent to ±0.025 mm
Density 2.20 g/cc Helium pycnometer
Hardness 85 Shore A ASTM D2240
Technical properties

After-processing / final-state properties

Typical installed and in-use properties for Tgon™ 805. Thermal resistance is reported at the stated interface pressure.

Property Value Unit Method / condition
Thermal conductivity, Z axis 5 W/m·K ASTM D5470, modified
Thermal conductivity, X-Y axis 240 W/m·K ASTM D5470, modified
Thermal resistance 0.07 °C·in²/W ASTM D5470, modified; 100 psi
Thermal resistance 0.42 °C·cm²/W ASTM D5470, modified; 681 kPa
Tensile strength 650 psi ASTM D412
Volume resistivity, in-plane 11 × 10−5 ohm·cm ASTM D257
Temperature range −240 to 300 °C Without adhesive; adhesive-backed material is rated 0 to 120°C
UL flammability rating V-0 — UL 94

Leading Brands Trust in Our Products and Services