Main features

  • 0.50 mm Thin-Gap Format
  • 10.2 W/m-K Thermal Conductivity
  • Non-Silicone Electrical Insulation

Product Description

Tflex SF10 0.50 mm Non-Silicone Thermal Gap Filler is a 229 x 229 mm ceramic-filled thermoplastic sheet for thin thermal interfaces in silicone-sensitive electronics. The 0.50 mm unreinforced construction provides 10.2 W/(m K) thermal conductivity and low thermal resistance while requiring limited pressure for surface contact. Its electrical insulation and -40 to 125 deg C operating range support controlled placement between heat-generating components and heat spreaders or housings. The material is supplied without fiberglass reinforcement and meets RoHS and REACH requirements. Applications include compact electronic assemblies that need a thin, non-silicone thermal gap-filling layer.

Key features

  • 0.50 mm Thin-Gap Format: The 229 x 229 mm sheet provides a controlled thin interface without fiberglass reinforcement.
  • 10.2 W/(m K) Thermal Conductivity: Ceramic-filled thermoplastic supports heat transfer across compact component gaps.
  • Non-Silicone Electrical Insulation: The formulation combines silicone-free handling with high volume resistivity.

Applications / Suitable for

  • Compact component-to-housing interfaces
  • Silicone-sensitive electronic assemblies
  • Thin converted thermal pads
Product Family

LAIRD TFLEX SF10.0.50

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Grey
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Ceramic filled non-silicone thermoplastic
Density (g)
3.7 g/cm3
Thermal Properties
Operating Temperature
(-)40 to 125 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
10 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Supplied 0.50 mm A18213-02 sheet configuration.

Property Value Unit Method / condition
Construction Ceramic-filled non-silicone thermoplastic No reinforcement carrier
Color Grey Visual
Nominal thickness 0.50 mm 0.020 inch
Sheet size 229 x 229 mm 9 x 9 inch sheet
Density 3.7 g/cc Helium pycnometer
Shelf life 2 years from shipment Specified shelf life
Technical properties

After-processing / final-state properties

Typical functional properties for the 0.50 mm A18213-02 configuration.

Property Value Unit Method / condition
Thermal conductivity 10.2 W/(m K) Hot Disk
Thermal resistance at 10 psi 0.05 C-in2/W 10 psi applied pressure
Thermal resistance at 30 to 50 psi 0.04 C-in2/W 30 to 50 psi applied pressure
Operating temperature range -40 to 125 deg C Laird test method
Dielectric constant 9 1 MHz; ASTM D150
Volume resistivity 1 x 10^14 ohm cm ASTM D257
Outgassing TML / CVCM 0.33 / 0.15 % ASTM E595